Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.653 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.072 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVO2 + V2H3O5 + Li3VO4 + H2O + N2 |
Band Gap2.462 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 290.5 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 258.0 |
BN (mp-984) | <1 0 1> | <1 0 1> | 141.8 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 244.5 |
MgO (mp-1265) | <1 1 0> | <1 -1 -1> | 153.8 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 244.5 |
C (mp-66) | <1 0 0> | <1 -1 -1> | 153.8 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 96.8 |
Mg (mp-153) | <1 0 1> | <1 -1 1> | 246.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 163.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 258.0 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 -1 -1> | 153.8 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 -1 -1> | 153.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 244.5 |
PbS (mp-21276) | <1 1 0> | <1 -1 -1> | 153.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 163.0 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 96.8 |
InP (mp-20351) | <1 1 0> | <1 -1 -1> | 153.8 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 1> | 141.8 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 -1> | 258.0 |
SiC (mp-11714) | <1 0 1> | <1 -1 0> | 226.3 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 290.5 |
Au (mp-81) | <1 1 0> | <0 1 1> | 148.2 |
Au (mp-81) | <1 1 1> | <0 0 1> | 244.5 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 163.0 |
WS2 (mp-224) | <0 0 1> | <0 1 0> | 96.8 |
Au (mp-81) | <1 0 0> | <1 -1 0> | 226.3 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 163.0 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 244.5 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 -1 -1> | 153.8 |
YAlO3 (mp-3792) | <0 1 0> | <1 -1 -1> | 153.8 |
CdWO4 (mp-19387) | <0 1 1> | <0 1 -1> | 200.7 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 244.5 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 216.6 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 244.5 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 108.3 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 244.5 |
ZnO (mp-2133) | <1 1 1> | <0 0 1> | 163.0 |
MgF2 (mp-1249) | <1 1 0> | <1 -1 0> | 226.3 |
Al2O3 (mp-1143) | <0 0 1> | <1 0 -1> | 258.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hg3SeO6 (mp-676169) | 0.6748 | 0.559 | 3 |
Ge7H18O23 (mp-627442) | 0.6322 | 0.093 | 3 |
Ge7H18O23 (mp-627418) | 0.6699 | 0.110 | 3 |
Hg3H4S2O11 (mp-721053) | 0.6014 | 0.003 | 4 |
ZnPH3O5 (mp-707311) | 0.5232 | 0.011 | 4 |
Co2P2H4O9 (mp-541410) | 0.5979 | 0.007 | 4 |
Fe2P2H4O9 (mp-541954) | 0.6094 | 0.000 | 4 |
Zn2P2H12O11 (mp-696085) | 0.5696 | 0.021 | 4 |
CuH20S2(NO7)2 (mp-722963) | 0.5545 | 0.281 | 5 |
Ga2P2H9NO11 (mp-705497) | 0.4942 | 0.073 | 5 |
CrP2H17N4O9 (mp-735484) | 0.5683 | 0.030 | 5 |
Cu2GeP2(H5O7)2 (mp-604273) | 0.5450 | 0.011 | 5 |
CoP2H17N4O9 (mp-744527) | 0.5442 | 0.056 | 5 |
CoMo8H36C8(NO16)2 (mp-745098) | 0.7030 | 0.197 | 6 |
Na4TeMo6H40(NO20)2 (mp-744242) | 0.6679 | 0.517 | 6 |
NiH32C8S4(NO5)2 (mp-579895) | 0.6514 | 0.150 | 6 |
LiH8C2S2NO5 (mp-605006) | 0.6798 | 0.196 | 6 |
MnH16C4N(OF2)2 (mp-743971) | 0.6303 | 0.170 | 6 |
NaAgH16C4S4(NO5)2 (mp-605018) | 0.7262 | 0.215 | 7 |
Na5P3H48C4N(O9F)3 (mp-738718) | 0.5999 | 0.047 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv H N O |
Final Energy/Atom-5.9595 eV |
Corrected Energy-579.8630 eV
-579.8630 eV = -536.3559 eV (uncorrected energy) - 26.6870 eV (MP Anion Correction) - 16.8200 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)