Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.666 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.689 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnCO3 + H2O + CO2 + C |
Band Gap2.848 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 265.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 332.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 265.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 332.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 199.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 332.3 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 232.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 332.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 265.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 332.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 332.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 332.3 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 332.3 |
InAs (mp-20305) | <1 1 0> | <1 1 1> | 262.6 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 232.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 66.5 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 258.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 66.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 66.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 332.3 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 265.8 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 332.3 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 199.4 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 332.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 199.4 |
BN (mp-984) | <0 0 1> | <1 1 1> | 131.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 332.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 199.4 |
BN (mp-984) | <1 1 0> | <1 0 1> | 136.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 332.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 332.3 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 332.3 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 332.3 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 265.8 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 332.3 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 1> | 245.9 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 265.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 332.3 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 332.3 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 332.3 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 332.3 |
PbS (mp-21276) | <1 1 0> | <1 1 1> | 262.6 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 332.3 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 258.4 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 232.6 |
Si (mp-149) | <1 1 0> | <0 0 1> | 332.3 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 332.3 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 332.3 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 332.3 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 332.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SbKrF7 (mp-30011) | 0.5985 | 0.000 | 3 |
SbKr3F11 (mp-30013) | 0.6028 | 0.006 | 3 |
RuXeF7 (mp-27288) | 0.5732 | 0.000 | 3 |
Sb2(KrF4)5 (mp-559168) | 0.6071 | 0.006 | 3 |
CrXeF6 (mp-558341) | 0.5597 | 0.000 | 3 |
ReH(CO)4 (mp-705527) | 0.5205 | 0.272 | 4 |
CS2NF5 (mp-555513) | 0.5530 | 0.253 | 4 |
MgAs2(XeF5)4 (mp-555546) | 0.4680 | 0.000 | 4 |
CuSb2(XeF8)2 (mp-606617) | 0.5869 | 0.000 | 4 |
NbSNCl6 (mp-608398) | 0.6063 | 0.091 | 4 |
TiF4 (mp-28974) | 0.7389 | 0.000 | 2 |
WN18 (mp-672264) | 0.6657 | 0.285 | 2 |
MnTeC5O6F5 (mp-650943) | 0.5260 | 0.493 | 5 |
MgAs2S2(OF3)4 (mp-555121) | 0.6026 | 0.052 | 5 |
CSNOF5 (mp-672266) | 0.5771 | 0.247 | 5 |
Sb2OsC4(OF3)4 (mp-559010) | 0.5193 | 0.057 | 5 |
Sb3C2N(OF8)2 (mp-566334) | 0.6062 | 0.078 | 5 |
Sb4IrC5ClO5F22 (mp-555612) | 0.6927 | 0.108 | 6 |
Tl2HPtC5N5O (mp-601902) | 0.6144 | 0.248 | 6 |
ReAsC5SNO5F7 (mp-565400) | 0.5745 | 0.168 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv H C O |
Final Energy/Atom-7.1268 eV |
Corrected Energy-454.1018 eV
Uncorrected energy = -427.6058 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Composition-based energy adjustment (-1.668 eV/atom x 6.0 atoms) = -10.0080 eV
Corrected energy = -454.1018 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)