material

RbCuO2

ID:

mp-7467

DOI:

10.17188/1288460


Tags: Rubidium dioxocuprate(III)

Material Details

Final Magnetic Moment
0.016 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.365 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.71 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.973 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmcm [63]
Hall
-C 2c 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 15096 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdWO4 (mp-19387) <1 1 1> <0 1 1> 0.004 259.4
C (mp-48) <0 0 1> <0 1 0> 0.004 190.2
CaF2 (mp-2741) <1 0 0> <1 1 0> 0.005 213.3
GdScO3 (mp-5690) <0 1 1> <0 1 0> 0.008 54.3
BaTiO3 (mp-5986) <1 0 1> <0 1 1> 0.008 324.2
GdScO3 (mp-5690) <1 0 0> <0 1 1> 0.008 324.2
GaP (mp-2490) <1 0 0> <1 1 0> 0.009 213.3
SiC (mp-7631) <1 0 0> <0 0 1> 0.009 235.5
Te2W (mp-22693) <1 0 0> <0 0 1> 0.009 294.4
TbScO3 (mp-31119) <1 0 0> <0 1 1> 0.016 324.2
Mg (mp-153) <1 0 1> <1 0 1> 0.016 264.7
CdWO4 (mp-19387) <1 0 1> <1 0 1> 0.021 88.2
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.021 294.4
ZrO2 (mp-2858) <1 1 0> <1 1 1> 0.023 276.9
LiF (mp-1138) <1 0 0> <1 1 1> 0.026 184.6
CdWO4 (mp-19387) <0 1 1> <1 1 0> 0.026 284.4
ZrO2 (mp-2858) <1 1 -1> <0 1 0> 0.027 135.8
YVO4 (mp-19133) <1 0 0> <0 1 0> 0.029 326.0
DyScO3 (mp-31120) <1 0 0> <0 1 1> 0.031 324.2
TbScO3 (mp-31119) <0 1 1> <0 1 0> 0.035 54.3
SiO2 (mp-6930) <1 1 0> <1 1 0> 0.036 142.2
TbScO3 (mp-31119) <0 1 0> <1 0 0> 0.036 131.4
Mg (mp-153) <0 0 1> <0 1 0> 0.040 190.2
LiF (mp-1138) <1 1 1> <0 1 1> 0.040 259.4
ZnO (mp-2133) <1 0 1> <1 0 0> 0.041 197.1
GdScO3 (mp-5690) <0 1 0> <1 0 0> 0.041 131.4
Ni (mp-23) <1 1 1> <0 0 1> 0.043 294.4
WS2 (mp-224) <1 0 1> <0 1 0> 0.044 326.0
LiGaO2 (mp-5854) <1 1 1> <1 1 1> 0.044 276.9
BN (mp-984) <0 0 1> <0 0 1> 0.045 235.5
MgF2 (mp-1249) <1 1 1> <0 1 0> 0.045 271.7
CdS (mp-672) <0 0 1> <0 1 0> 0.046 244.5
WS2 (mp-224) <0 0 1> <1 1 0> 0.049 71.1
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.049 71.1
LiGaO2 (mp-5854) <1 0 1> <0 1 0> 0.049 135.8
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.049 71.1
Bi2Se3 (mp-541837) <0 0 1> <0 1 0> 0.052 244.5
GaN (mp-804) <1 1 1> <0 1 0> 0.053 217.3
AlN (mp-661) <1 0 1> <0 0 1> 0.053 176.6
SiO2 (mp-6930) <1 0 0> <0 1 0> 0.055 27.2
LaF3 (mp-905) <1 0 0> <1 0 1> 0.055 264.7
TiO2 (mp-390) <1 0 0> <0 1 1> 0.056 259.4
BN (mp-984) <1 0 0> <0 1 0> 0.059 190.2
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.060 294.4
Ga2O3 (mp-886) <1 1 0> <0 0 1> 0.061 294.4
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.061 294.4
TiO2 (mp-390) <0 0 1> <0 1 0> 0.063 190.2
BaTiO3 (mp-5986) <1 0 0> <1 1 1> 0.064 184.6
AlN (mp-661) <1 0 0> <0 1 0> 0.064 108.7
Al (mp-134) <1 0 0> <0 0 1> 0.068 294.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
154 22 13 0 0 0
22 60 22 0 0 0
13 22 27 0 0 0
0 0 0 9 0 0
0 0 0 0 7 0
0 0 0 0 0 13
Compliance Tensor Sij (10-12Pa-1)
6.9 -1.9 -1.7 0 0 0
-1.9 24.2 -18.6 0 0 0
-1.7 -18.6 52.5 0 0 0
0 0 0 116.3 0 0
0 0 0 0 147.5 0
0 0 0 0 0 76.8
Shear Modulus GV
18 GPa
Bulk Modulus KV
39 GPa
Shear Modulus GR
10 GPa
Bulk Modulus KR
26 GPa
Shear Modulus GVRH
14 GPa
Bulk Modulus KVRH
32 GPa
Elastic Anisotropy
4.20
Poisson's Ratio
0.31

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
6.77 0.00 0.00
0.00 3.03 -0.00
0.00 -0.00 2.33
Dielectric Tensor εij (total)
8.56 0.00 0.00
0.00 5.11 -0.00
0.00 -0.00 4.61
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.04
Polycrystalline dielectric constant εpoly
(total)
6.09
Refractive Index n
2.01
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CsAuO2 (mp-997024) 0.2313 0.000 3
RbFeO2 (mp-770384) 0.1326 0.158 3
KCuO2 (mp-3982) 0.1879 0.000 3
CsCuO2 (mp-553310) 0.1729 0.000 3
CsAgO2 (mp-1096933) 0.1447 0.000 3
K3LiIrO4 (mp-561288) 0.6502 0.002 4
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Rb_sv Cu_pv O
Final Energy/Atom
-4.7581 eV
Corrected Energy
-40.8128 eV
Uncorrected energy = -38.0648 eV Composition-based energy adjustment (-0.687 eV/atom x 4.0 atoms) = -2.7480 eV Corrected energy = -40.8128 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 15096
Submitted by
User remarks:
  • Rubidium dioxocuprate(III)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)