Final Magnetic Moment0.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.744 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.024 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSrI2 + BaI2 |
Band Gap3.769 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP42/mnm [136] |
Hall-P 4n 2n |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BN (mp-984) | <1 0 1> | <0 0 1> | 255.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 319.6 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 249.7 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 191.7 |
C (mp-66) | <1 0 0> | <0 0 1> | 63.9 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 1> | 140.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 191.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 63.9 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 140.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 319.6 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 249.7 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 319.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 319.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 319.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 255.6 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 176.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 319.6 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 176.6 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 1> | 140.3 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 319.6 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 63.9 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 1> | 140.3 |
NdGaO3 (mp-3196) | <1 0 0> | <1 1 0> | 176.6 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 1> | 140.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 187.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 127.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 140.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 319.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 63.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 319.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 63.9 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 140.3 |
MoSe2 (mp-1634) | <1 1 0> | <1 1 0> | 176.6 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 319.6 |
Au (mp-81) | <1 0 0> | <0 0 1> | 319.6 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 319.6 |
WS2 (mp-224) | <0 0 1> | <1 1 0> | 176.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 63.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 319.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 319.6 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 319.6 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 255.6 |
WS2 (mp-224) | <1 1 0> | <0 0 1> | 319.6 |
WS2 (mp-224) | <1 1 1> | <0 0 1> | 319.6 |
C (mp-48) | <1 0 0> | <0 0 1> | 191.7 |
C (mp-48) | <1 0 1> | <0 0 1> | 255.6 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 191.7 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 63.9 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 140.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 255.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.00000 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.17 | 0.00 | 0.00 |
0.00 | 3.17 | 0.00 |
0.00 | 0.00 | 3.30 |
Dielectric Tensor εij (total) |
||
---|---|---|
9.00 | 0.00 | 0.00 |
0.00 | 9.00 | 0.00 |
0.00 | 0.00 | 6.57 |
Polycrystalline dielectric constant
εpoly∞
3.22
|
Polycrystalline dielectric constant
εpoly
8.19
|
Refractive Index n1.79 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr2WO6 (mp-774203) | 0.0748 | 0.000 | 3 |
Ga2WO6 (mp-770737) | 0.0967 | 0.043 | 3 |
Li2MoF6 (mp-615064) | 0.1004 | 0.000 | 3 |
Li2PtF6 (mp-13986) | 0.1040 | 0.000 | 3 |
Li2PdF6 (mp-13985) | 0.0949 | 0.000 | 3 |
Ta2CrNO5 (mp-782717) | 0.2110 | 0.064 | 4 |
LiFe3(OF3)2 (mp-779990) | 0.2158 | 0.007 | 4 |
Ta2CrNO5 (mp-849938) | 0.1993 | 0.067 | 4 |
Ta2CrNO5 (mp-849666) | 0.2007 | 0.073 | 4 |
Ta2CrNO5 (mp-849504) | 0.1681 | 0.061 | 4 |
TiO2 (mvc-6590) | 0.1755 | 0.037 | 2 |
RhCl2 (mp-867259) | 0.1867 | 0.195 | 2 |
VO2 (mp-19094) | 0.1852 | 0.000 | 2 |
MoO2 (mp-715476) | 0.1777 | 0.000 | 2 |
WO2 (mp-715508) | 0.1727 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Sr_sv I |
Final Energy/Atom-3.3744 eV |
Corrected Energy-60.7396 eV
-60.7396 eV = -60.7396 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)