material

BaCuO2

ID:

mp-752398

DOI:

10.17188/1272676


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.922 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.077 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.16 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
BaCuO2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/mmm [123]
Hall
-P 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
NaCl (mp-22862) <1 0 0> <0 0 1> 0.000 32.4
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.001 145.8
NaCl (mp-22862) <1 1 1> <1 0 0> 0.001 280.9
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.006 16.2
SiC (mp-7631) <0 0 1> <1 0 0> 0.006 124.8
SiC (mp-11714) <0 0 1> <1 0 0> 0.008 124.8
Si (mp-149) <1 1 1> <1 0 0> 0.009 156.1
CeO2 (mp-20194) <1 1 1> <1 0 0> 0.012 156.1
MgO (mp-1265) <1 0 0> <0 0 1> 0.022 145.8
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.029 46.8
BaTiO3 (mp-5986) <1 0 0> <1 0 1> 0.031 67.5
Al (mp-134) <1 0 0> <0 0 1> 0.032 16.2
Ge(Bi3O5)4 (mp-23352) <1 0 0> <0 0 1> 0.034 210.6
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.037 210.6
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.044 265.3
GaP (mp-2490) <1 1 1> <1 0 0> 0.049 156.1
CdS (mp-672) <1 1 0> <1 0 0> 0.053 296.5
Cu (mp-30) <1 0 0> <0 0 1> 0.055 64.8
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.059 324.0
Cu (mp-30) <1 1 1> <1 0 0> 0.062 249.7
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.063 64.8
KCl (mp-23193) <1 0 0> <0 0 1> 0.065 81.0
ZrO2 (mp-2858) <0 1 1> <1 0 1> 0.068 157.5
AlN (mp-661) <1 0 1> <1 1 0> 0.069 88.3
MgAl2O4 (mp-3536) <1 1 1> <1 0 0> 0.077 234.1
Ga2O3 (mp-886) <1 1 0> <1 1 0> 0.080 220.7
PbS (mp-21276) <1 0 0> <0 0 1> 0.082 145.8
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.083 16.2
Fe2O3 (mp-24972) <0 0 1> <1 0 0> 0.085 249.7
CdWO4 (mp-19387) <0 1 0> <1 1 0> 0.089 132.4
WS2 (mp-224) <1 1 0> <1 0 1> 0.091 157.5
TeO2 (mp-2125) <1 0 1> <1 1 0> 0.092 154.5
CaF2 (mp-2741) <1 1 1> <1 0 0> 0.092 156.1
TiO2 (mp-390) <1 1 0> <1 0 0> 0.096 156.1
SiC (mp-8062) <1 1 1> <1 0 0> 0.101 327.7
CdS (mp-672) <1 0 0> <1 0 0> 0.103 171.7
PbS (mp-21276) <1 1 0> <1 0 1> 0.106 202.4
LiGaO2 (mp-5854) <1 1 0> <1 1 0> 0.110 286.9
LaAlO3 (mp-2920) <1 1 0> <1 0 1> 0.116 247.4
TiO2 (mp-390) <1 0 0> <1 1 1> 0.121 109.5
C (mp-66) <1 0 0> <0 0 1> 0.128 64.8
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.129 249.7
BN (mp-984) <1 0 0> <0 0 1> 0.134 97.2
SiC (mp-11714) <1 0 1> <1 1 1> 0.135 355.9
ZnO (mp-2133) <1 1 1> <1 0 1> 0.135 224.9
MoSe2 (mp-1634) <1 1 0> <1 1 0> 0.142 88.3
ZnSe (mp-1190) <1 1 1> <1 0 0> 0.148 280.9
C (mp-48) <1 1 0> <1 0 0> 0.148 265.3
DyScO3 (mp-31120) <1 0 1> <1 1 1> 0.149 54.8
CdS (mp-672) <1 1 1> <0 0 1> 0.149 210.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
160 48 48 0 0 0
48 177 89 0 0 0
48 89 177 0 0 0
0 0 0 67 0 0
0 0 0 0 49 0
0 0 0 0 0 49
Compliance Tensor Sij (10-12Pa-1)
7 -1.3 -1.3 0 0 0
-1.3 7.8 -3.6 0 0 0
-1.3 -3.6 7.8 0 0 0
0 0 0 14.9 0 0
0 0 0 0 20.3 0
0 0 0 0 0 20.3
Shear Modulus GV
55 GPa
Bulk Modulus KV
98 GPa
Shear Modulus GR
53 GPa
Bulk Modulus KR
96 GPa
Shear Modulus GVRH
54 GPa
Bulk Modulus KVRH
97 GPa
Elastic Anisotropy
0.18
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
SrFeO2 (mp-24964) 0.4967 0.002 3
SrCuO2 (mp-37514) 0.3696 0.014 3
MgNiH2 (mp-1017509) 0.1718 0.030 3
BaAgO2 (mp-996990) 0.4746 0.000 3
BaCuS2 (mp-1096843) 0.1766 0.092 3
Ba2Pd(OF)2 (mp-6123) 0.5521 0.052 4
Sr2Cu(OF)2 (mp-1025280) 0.6252 0.027 4
LiLa4AuO8 (mp-560605) 0.7227 0.000 4
BaTi2Bi2O (mp-1070808) 0.6802 0.020 4
BaTi2Sb2O (mp-1070806) 0.6430 0.000 4
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Cu_pv O
Final Energy/Atom
-5.5497 eV
Corrected Energy
-23.6032 eV
-23.6032 eV = -22.1987 eV (uncorrected energy) - 1.4046 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations