Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.256 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.002 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.59 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRbTmO2 + Rb2O |
Band Gap2.172 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 1> | 109.9 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 186.0 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 175.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 234.4 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 253.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 279.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 258.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 175.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 234.4 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 234.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 293.0 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 100.6 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 107.8 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 215.6 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 293.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 107.8 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 234.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 215.6 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 215.6 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 253.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 293.0 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 279.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 175.8 |
BN (mp-984) | <1 0 0> | <1 0 0> | 172.4 |
BN (mp-984) | <1 0 1> | <0 1 0> | 279.0 |
BN (mp-984) | <1 1 1> | <0 0 1> | 234.4 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 234.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 293.0 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 234.4 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 215.6 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 258.7 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 293.0 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 234.4 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 234.4 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 279.0 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 175.8 |
C (mp-66) | <1 0 0> | <1 0 1> | 215.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 293.0 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 258.7 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 175.8 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 234.4 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 253.6 |
LaF3 (mp-905) | <1 0 0> | <1 0 1> | 107.8 |
LaF3 (mp-905) | <1 0 1> | <0 1 0> | 279.0 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 175.8 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 258.7 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 175.8 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 234.4 |
InSb (mp-20012) | <1 0 0> | <1 0 1> | 215.6 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 293.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb3YO3 (mp-756474) | 0.0947 | 0.010 | 3 |
Rb3LuO3 (mp-772821) | 0.0801 | 0.000 | 3 |
Rb3HoO3 (mp-779144) | 0.0554 | 0.007 | 3 |
Rb3DyO3 (mp-778968) | 0.0757 | 0.010 | 3 |
Rb3ErO3 (mp-756812) | 0.0595 | 0.005 | 3 |
LiSiBiO4 (mp-757219) | 0.5915 | 0.093 | 4 |
LiFePO4 (mp-766762) | 0.5027 | 0.544 | 4 |
Cs2Na3InO4 (mp-504852) | 0.5760 | 0.000 | 4 |
CsGeBiS4 (mp-553970) | 0.5594 | 0.000 | 4 |
K3LiSiO4 (mp-561474) | 0.4965 | 0.000 | 4 |
Sr2YAlW2O7 (mvc-356) | 0.7212 | 0.551 | 5 |
Sr2YAlSn2O7 (mvc-10827) | 0.7435 | 0.245 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Tm_3 O |
Final Energy/Atom-5.1350 eV |
Corrected Energy-152.0231 eV
Uncorrected energy = -143.7791 eV
Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV
Corrected energy = -152.0231 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)