Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.252 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.534 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 254.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 169.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 169.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 275.5 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 226.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 254.6 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 56.6 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 339.4 |
YVO4 (mp-19133) | <1 1 0> | <1 0 -1> | 252.2 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 226.3 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 127.3 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 282.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 282.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 275.5 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 282.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 254.6 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 127.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 169.7 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 226.3 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 339.4 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 339.4 |
Al (mp-134) | <1 1 0> | <1 0 1> | 254.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 169.7 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 226.3 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 282.9 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 282.9 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 226.3 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 127.3 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 207.9 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 226.3 |
Mg (mp-153) | <1 0 1> | <1 0 -1> | 168.2 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 282.9 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 282.9 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 207.9 |
TiO2 (mp-2657) | <1 1 0> | <1 0 -1> | 252.2 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 183.7 |
C (mp-66) | <1 0 0> | <1 0 0> | 282.9 |
Ni (mp-23) | <1 1 0> | <0 1 1> | 138.7 |
InSb (mp-20012) | <1 1 0> | <1 0 1> | 127.3 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 169.7 |
GaP (mp-2490) | <1 1 1> | <1 0 1> | 254.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 183.7 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 339.4 |
Ga2O3 (mp-886) | <1 0 0> | <1 1 0> | 236.7 |
Si (mp-149) | <1 1 1> | <1 0 1> | 254.6 |
Au (mp-81) | <1 1 0> | <0 0 1> | 275.5 |
Au (mp-81) | <1 1 1> | <1 0 0> | 282.9 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 169.7 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 226.3 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 169.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.66 | 0.00 | -0.03 |
0.00 | 2.71 | -0.00 |
-0.03 | -0.00 | 2.65 |
Dielectric Tensor εij (total) |
||
---|---|---|
6.77 | 0.00 | -0.20 |
0.00 | 10.13 | -0.00 |
-0.20 | -0.00 | 6.74 |
Polycrystalline dielectric constant
εpoly∞
2.68
|
Polycrystalline dielectric constant
εpoly
7.88
|
Refractive Index n1.64 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb2WO4 (mp-18864) | 0.1494 | 0.000 | 3 |
K2WO4 (mp-18780) | 0.3019 | 0.000 | 3 |
K2MoO4 (mp-18914) | 0.2695 | 0.000 | 3 |
Rb2MoO4 (mp-19212) | 0.1218 | 0.000 | 3 |
P2Pb3S8 (mp-28140) | 0.4445 | 0.000 | 3 |
KPPbS4 (mp-638150) | 0.4543 | 0.000 | 4 |
KSrVO4 (mp-628859) | 0.5042 | 0.000 | 4 |
RbEuPO4 (mp-18169) | 0.4614 | 0.015 | 4 |
Pb2S(O2F)2 (mp-557531) | 0.4093 | 0.000 | 4 |
KEuPS4 (mp-628735) | 0.4834 | 0.000 | 4 |
Ga2I3 (mp-636675) | 0.6667 | 0.000 | 2 |
GaBr2 (mp-650841) | 0.5629 | 0.011 | 2 |
SiI2 (mp-541053) | 0.6950 | 0.026 | 2 |
CuCl4 (mp-32829) | 0.6871 | 0.099 | 2 |
VCl4 (mp-570763) | 0.6484 | 0.004 | 2 |
KBiS(ClO2)2 (mp-23645) | 0.4877 | 0.000 | 5 |
RbHoHS2O9 (mp-761809) | 0.6540 | 0.080 | 5 |
K2YbMoPO8 (mp-565817) | 0.6280 | 0.003 | 5 |
NaYPO4F (mp-10804) | 0.6273 | 0.003 | 5 |
NaErPO4F (mp-10935) | 0.6304 | 0.004 | 5 |
Run TypeGGA+U |
Energy Cutoff700 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Cs_sv W_pv O |
Final Energy/Atom-6.1636 eV |
Corrected Energy-100.6622 eV
Uncorrected energy = -86.2902 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Composition-based energy adjustment (-4.438 eV/atom x 2.0 atoms) = -8.8760 eV
Corrected energy = -100.6622 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)