Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.166 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.012 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIma2 [46] |
HallI 2 2a |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 246.8 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 175.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 164.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 246.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 246.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 173.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 246.8 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 246.8 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 1> | 175.7 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 191.6 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 155.2 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 173.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 164.5 |
C (mp-66) | <1 1 1> | <0 1 1> | 175.7 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 164.5 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 246.8 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 155.2 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 246.8 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 246.8 |
InSb (mp-20012) | <1 1 0> | <1 0 1> | 191.6 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 155.2 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 164.5 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 155.2 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 164.5 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 164.5 |
Au (mp-81) | <1 0 0> | <0 0 1> | 246.8 |
Au (mp-81) | <1 1 0> | <0 0 1> | 246.8 |
CdSe (mp-2691) | <1 0 0> | <0 1 0> | 155.2 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 164.5 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 246.8 |
CaCO3 (mp-3953) | <0 0 1> | <0 1 1> | 175.7 |
SiC (mp-8062) | <1 0 0> | <1 0 1> | 191.6 |
GaSb (mp-1156) | <1 0 0> | <0 1 0> | 155.2 |
ZnO (mp-2133) | <1 0 0> | <0 1 1> | 175.7 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 164.5 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 164.5 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 246.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaLaCl5 (mp-772035) | 0.6142 | 0.062 | 3 |
BaYbSn3 (mp-571479) | 0.4649 | 0.000 | 3 |
Cs5(KPb6)3 (mp-581775) | 0.5971 | 0.006 | 3 |
BaCaSn3 (mp-583645) | 0.4628 | 0.000 | 3 |
K3Ge4Au (mp-17112) | 0.6174 | 0.000 | 3 |
RbHfAgTe3 (mp-9780) | 0.7222 | 0.000 | 4 |
MgSi (mp-1073812) | 0.5442 | 0.172 | 2 |
Mg4Si3 (mp-1074573) | 0.5235 | 0.200 | 2 |
Mg3Si4 (mp-1075302) | 0.4895 | 0.252 | 2 |
Mg5Si6 (mp-1075464) | 0.5602 | 0.237 | 2 |
Mg3Si2 (mp-1075790) | 0.5550 | 0.137 | 2 |
Rb (mp-640416) | 0.7415 | 0.057 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Na_pv Si |
Final Energy/Atom-3.9184 eV |
Corrected Energy-109.7144 eV
-109.7144 eV = -109.7144 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)