Final Magnetic Moment14.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.688 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.056 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaO + Gd2O3 |
Band Gap3.260 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 191.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 287.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 191.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 287.5 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 287.5 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 287.5 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 287.5 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 191.7 |
WS2 (mp-224) | <1 0 0> | <1 1 0> | 135.5 |
NaCl (mp-22862) | <1 1 0> | <1 1 0> | 135.5 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 287.5 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 95.8 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 191.7 |
Ge (mp-32) | <1 1 1> | <1 0 0> | 287.5 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 287.5 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 287.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 287.5 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 287.5 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 166.0 |
Al (mp-134) | <1 1 1> | <1 0 0> | 287.5 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 166.0 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 191.7 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 287.5 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 191.7 |
NaCl (mp-22862) | <1 1 1> | <1 1 1> | 166.0 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 287.5 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 191.7 |
SrTiO3 (mp-4651) | <1 0 0> | <1 1 0> | 135.5 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 191.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ga2CuO4 (mp-753397) | 0.0359 | 0.075 | 3 |
Cr2NiO4 (mp-566016) | 0.0433 | 0.199 | 3 |
CaTb2O4 (mp-755044) | 0.0415 | 0.049 | 3 |
CaSm2O4 (mp-754240) | 0.0265 | 0.077 | 3 |
CaY2O4 (mp-753815) | 0.0383 | 0.040 | 3 |
Li2TiFe3O8 (mp-850231) | 0.0666 | 0.030 | 4 |
Li2MnCo3O8 (mp-761737) | 0.0566 | 0.079 | 4 |
Li2Fe3CuO8 (mp-772689) | 0.0704 | 0.035 | 4 |
Li2V3CoO8 (mp-765546) | 0.0557 | 0.075 | 4 |
Li2Ti3CrO8 (mp-771759) | 0.0609 | 0.003 | 4 |
Co3O4 (mp-559191) | 0.1676 | 0.000 | 2 |
In3S4 (mp-556597) | 0.1154 | 0.048 | 2 |
Co3O4 (mp-18748) | 0.1191 | 0.000 | 2 |
Sn3N4 (mp-16031) | 0.1355 | 0.000 | 2 |
Ge3N4 (mp-476) | 0.1690 | 0.109 | 2 |
Li4Cr2Fe3Co3O16 (mp-775698) | 0.3851 | 0.130 | 5 |
Li4Mn2Fe3Co3O16 (mp-761441) | 0.3926 | 0.081 | 5 |
Li14Mn22Cr3Cu3O56 (mp-735790) | 0.3614 | 0.021 | 5 |
Li4Mn3Cr3(CuO8)2 (mp-765456) | 0.3610 | 0.072 | 5 |
Li4Cr3Cu3(SbO8)2 (mp-783908) | 0.3850 | 0.042 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Gd O |
Final Energy/Atom-10.4133 eV |
Corrected Energy-151.4046 eV
-151.4046 eV = -145.7863 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)