Final Magnetic Moment0.026 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.682 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.057 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.40 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSrI2 + BaI2 |
Band Gap3.252 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 199.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 199.4 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 163.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 163.1 |
YVO4 (mp-19133) | <1 1 1> | <1 0 -1> | 163.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 299.1 |
C (mp-66) | <1 1 0> | <1 0 0> | 181.9 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 -1> | 163.1 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 299.1 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 299.1 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 -1> | 163.1 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 199.4 |
SiC (mp-11714) | <1 1 0> | <1 0 -1> | 163.1 |
Au (mp-81) | <1 1 1> | <1 0 0> | 181.9 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 199.4 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 299.1 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 0> | 181.9 |
Cu (mp-30) | <1 1 1> | <1 0 0> | 181.9 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 199.4 |
ZnO (mp-2133) | <1 1 1> | <0 1 1> | 190.5 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 199.4 |
Fe2O3 (mp-24972) | <0 0 1> | <1 0 0> | 181.9 |
Fe2O3 (mp-24972) | <1 0 1> | <0 0 1> | 299.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3AlTe3 (mp-9680) | 0.6272 | 0.000 | 3 |
Zr6Nb2O17 (mp-766207) | 0.6486 | 0.039 | 3 |
Ba2LaI7 (mp-772158) | 0.6371 | 0.054 | 3 |
BaCa2I6 (mp-766332) | 0.6306 | 0.094 | 3 |
Sm3(Sb7Te12)2 (mp-675760) | 0.6426 | 0.124 | 3 |
SrLi4NiO4 (mp-778288) | 0.7385 | 0.096 | 4 |
BaYbCdSb2 (mp-865143) | 0.7235 | 0.000 | 4 |
Ce3NbS3O4 (mp-683997) | 0.7474 | 0.067 | 4 |
Nb2Tl3CuSe12 (mp-570757) | 0.7370 | 0.000 | 4 |
Mg2Si3 (mp-1072989) | 0.5988 | 0.198 | 2 |
Mg2Si3 (mp-1073164) | 0.5539 | 0.128 | 2 |
Mg4Si3 (mp-1074404) | 0.5646 | 0.133 | 2 |
Mg5Si9 (mp-1075715) | 0.5815 | 0.197 | 2 |
MgSi2 (mp-1073408) | 0.5294 | 0.198 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Sr_sv I |
Final Energy/Atom-3.2864 eV |
Corrected Energy-118.3096 eV
-118.3096 eV = -118.3096 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)