Final Magnetic Moment1.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.844 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.047 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAgF2 + LiF + AgF |
Band Gap0.184 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 217.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 122.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 162.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 284.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 325.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 203.5 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 274.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 122.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 137.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 55.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 55.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 162.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 68.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 325.5 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 249.2 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 217.3 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 222.5 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 137.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 122.1 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 203.5 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 162.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 72.4 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 122.1 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 55.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 244.1 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 284.8 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 182.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 137.8 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 137.8 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 333.7 |
GaSe (mp-1943) | <1 0 1> | <0 1 0> | 278.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 284.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 55.6 |
BN (mp-984) | <1 0 0> | <1 0 0> | 289.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 244.1 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 284.8 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 166.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 122.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 122.1 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 122.1 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 217.3 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 72.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 284.8 |
Al (mp-134) | <1 1 1> | <0 1 0> | 55.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 166.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 111.2 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 137.8 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 144.9 |
BN (mp-984) | <0 0 1> | <1 0 0> | 217.3 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 122.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlMoO3 (mvc-15905) | 0.5039 | 0.295 | 3 |
Fe3(OF)2 (mp-767081) | 0.4797 | 0.044 | 3 |
Cr(AgO2)2 (mp-557056) | 0.4940 | 0.023 | 3 |
AlWO3 (mvc-4004) | 0.5158 | 0.280 | 3 |
Mn(AgO2)2 (mp-554049) | 0.3801 | 0.185 | 3 |
LiVSiO4 (mp-767049) | 0.3031 | 0.011 | 4 |
LiTiSiO4 (mp-753580) | 0.3469 | 0.086 | 4 |
LiCoSiO4 (mp-763500) | 0.2970 | 0.158 | 4 |
LiFeSiO4 (mp-861542) | 0.2799 | 0.181 | 4 |
LiMnSiO4 (mp-780533) | 0.2892 | 0.044 | 4 |
Mn3O4 (mp-715513) | 0.7304 | 0.000 | 2 |
Mn3O4 (mp-566607) | 0.7431 | 0.000 | 2 |
Mn3O4 (mp-18759) | 0.7435 | 0.000 | 2 |
Al2O3 (mp-7048) | 0.7431 | 0.009 | 2 |
Ga2O3 (mp-886) | 0.7440 | 0.000 | 2 |
Li4Mn3Nb3(TeO8)2 (mp-778817) | 0.6017 | 0.231 | 5 |
Li4Mn3Nb3(SbO8)2 (mp-773620) | 0.6026 | 0.172 | 5 |
Li4Nb2Fe3Te3O16 (mp-765556) | 0.5735 | 0.259 | 5 |
Li4Co3Cu3(WO8)2 (mp-763112) | 0.5983 | 0.068 | 5 |
Na2TiZn2SiO7 (mp-13810) | 0.5522 | 0.000 | 5 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.6606 | 0.008 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ag F |
Final Energy/Atom-3.7377 eV |
Corrected Energy-104.6560 eV
-104.6560 eV = -104.6560 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)