Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.453 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.060 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.10 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2CuP2O7 + CuO + Li3PO4 |
Band Gap0.632 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 200.7 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 299.4 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 -1> | 247.3 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 118.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 123.9 |
AlN (mp-661) | <1 0 1> | <1 -1 -1> | 91.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 247.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 173.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 118.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 123.9 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 266.2 |
GaAs (mp-2534) | <1 0 0> | <1 -1 0> | 228.8 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 229.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 222.9 |
BaF2 (mp-1029) | <1 0 0> | <0 1 -1> | 282.7 |
BaF2 (mp-1029) | <1 1 0> | <1 -1 0> | 267.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 123.9 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 118.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 173.4 |
GaN (mp-804) | <1 1 0> | <1 -1 1> | 90.2 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 118.8 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 289.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 172.1 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 231.8 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 258.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 247.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 123.9 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 297.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 123.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 222.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 266.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 229.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 343.2 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 1> | 289.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 299.4 |
InAs (mp-20305) | <1 1 0> | <1 -1 0> | 267.0 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 322.3 |
ZnSe (mp-1190) | <1 0 0> | <1 -1 0> | 228.8 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 222.9 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 222.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 198.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 222.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 343.2 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 200.7 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 118.8 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 200.7 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 198.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 222.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 322.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 222.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb4PbO4 (mp-771328) | 0.6833 | 0.011 | 3 |
Cs4PbO4 (mp-542099) | 0.7304 | 0.000 | 3 |
Na6Ti2O7 (mp-778364) | 0.7210 | 0.004 | 3 |
Na3Mo2N5 (mp-1029845) | 0.6368 | 0.000 | 3 |
Na3W2N5 (mp-1029565) | 0.6639 | 0.000 | 3 |
Li2VSiO4 (mp-767138) | 0.6215 | 0.084 | 4 |
Li3FeBO4 (mp-778748) | 0.5826 | 0.188 | 4 |
Li4Fe(PO4)2 (mp-772126) | 0.2461 | 0.053 | 4 |
Na4Cu(AsO4)2 (mp-555821) | 0.4434 | 0.016 | 4 |
Cd2Cu(PO4)2 (mp-13361) | 0.5994 | 0.000 | 4 |
Li5Fe4P4O16F (mp-762773) | 0.7152 | 0.310 | 5 |
Rb5LiSi2NiO8 (mp-652260) | 0.7168 | 0.018 | 5 |
Sr2AlV2GaO7 (mvc-350) | 0.7472 | 0.325 | 5 |
Na3Li2Al(SiO4)2 (mp-1020163) | 0.6973 | 0.000 | 5 |
Li2PWO4F (mp-25728) | 0.7073 | 0.352 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv P O |
Final Energy/Atom-6.2212 eV |
Corrected Energy-98.9359 eV
-98.9359 eV = -93.3176 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)