material

NaTiS2

ID:

mp-752947

DOI:

10.17188/1288855


Material Details

Final Magnetic Moment
0.867 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-1.673 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.007 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.01 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
NaTiS2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.002 76.6
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.002 10.9
Si (mp-149) <1 1 1> <0 0 1> 0.004 207.9
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.005 207.9
Te2Mo (mp-602) <1 1 0> <0 0 1> 0.008 284.5
InSb (mp-20012) <1 1 1> <0 0 1> 0.009 76.6
CdTe (mp-406) <1 1 1> <0 0 1> 0.014 76.6
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.016 76.6
LiTaO3 (mp-3666) <1 0 0> <1 0 1> 0.020 291.8
LiF (mp-1138) <1 1 0> <1 0 1> 0.025 212.2
CdS (mp-672) <1 0 1> <1 0 1> 0.027 291.8
Ag (mp-124) <1 1 1> <0 0 1> 0.030 207.9
SiC (mp-11714) <1 0 0> <1 1 0> 0.032 125.6
BN (mp-984) <1 1 1> <0 0 1> 0.033 339.2
Mg (mp-153) <1 0 0> <1 1 1> 0.033 216.3
SiC (mp-11714) <0 0 1> <0 0 1> 0.035 32.8
GaP (mp-2490) <1 1 1> <0 0 1> 0.036 207.9
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.037 207.9
SiC (mp-7631) <1 0 0> <0 0 1> 0.037 186.0
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.038 207.9
SiC (mp-7631) <0 0 1> <0 0 1> 0.039 32.8
YAlO3 (mp-3792) <1 1 1> <1 1 0> 0.039 125.6
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.040 217.5
SiC (mp-11714) <1 1 1> <1 0 0> 0.041 217.5
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.044 186.0
MoS2 (mp-1434) <1 0 0> <0 0 1> 0.044 273.6
GaN (mp-804) <1 1 1> <0 0 1> 0.045 153.2
LiGaO2 (mp-5854) <1 1 0> <1 0 1> 0.046 291.8
CdSe (mp-2691) <1 1 0> <1 0 0> 0.048 217.5
SiC (mp-8062) <1 1 1> <0 0 1> 0.049 32.8
TiO2 (mp-390) <0 0 1> <0 0 1> 0.052 229.8
YAlO3 (mp-3792) <1 0 0> <1 0 1> 0.060 79.6
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.061 207.9
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.065 207.9
Ge (mp-32) <1 1 1> <0 0 1> 0.070 175.1
Mg (mp-153) <1 1 1> <0 0 1> 0.071 153.2
Ge3(BiO3)4 (mp-23560) <1 1 0> <1 0 1> 0.072 159.2
Au (mp-81) <1 1 1> <0 0 1> 0.073 207.9
ZrO2 (mp-2858) <1 0 -1> <1 0 0> 0.083 72.5
LiF (mp-1138) <1 0 0> <1 0 1> 0.085 185.7
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.086 197.0
TiO2 (mp-390) <1 1 1> <1 0 0> 0.088 217.5
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.089 229.8
KP(HO2)2 (mp-23959) <0 1 0> <1 1 1> 0.095 302.8
C (mp-48) <0 0 1> <0 0 1> 0.099 98.5
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.100 217.5
LiNbO3 (mp-3731) <1 0 0> <1 0 1> 0.108 291.8
SiC (mp-7631) <1 1 0> <0 0 1> 0.109 164.1
Ni (mp-23) <1 0 0> <0 0 1> 0.112 87.5
Ni (mp-23) <1 1 0> <1 0 1> 0.116 53.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
101 16 34 -3 0 0
16 101 34 3 0 0
34 34 118 0 0 0
-3 3 0 31 0 0
0 0 0 0 31 -3
0 0 0 0 -3 42
Compliance Tensor Sij (10-12Pa-1)
11.1 -0.8 -3 1.3 0 0
-0.8 11.1 -3 -1.3 0 0
-3 -3 10.2 0 0 0
1.3 -1.3 0 32.2 0 0
0 0 0 0 32.2 2.6
0 0 0 0 2.6 23.8
Shear Modulus GV
37 GPa
Bulk Modulus KV
54 GPa
Shear Modulus GR
36 GPa
Bulk Modulus KR
53 GPa
Shear Modulus GVRH
36 GPa
Bulk Modulus KVRH
54 GPa
Elastic Anisotropy
0.18
Poisson's Ratio
0.22

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TlCdS2 (mp-7708) 0.3657 0.168 3
NaCrS2 (mp-637292) 0.2899 0.005 3
NaVS2 (mp-999454) 0.2191 0.092 3
NaVO2 (mp-770068) 0.3261 0.067 3
CaTiS2 (mvc-16021) 0.3232 0.269 3
Na3Ni2SbO6 (mp-971678) 0.4662 0.000 4
Na5Li4Ti5O14 (mp-775424) 0.5662 0.017 4
Na2Li(NiO2)3 (mp-773956) 0.5436 0.031 4
Na3Co2SbO6 (mp-561940) 0.4895 0.015 4
Na3Co2SbO6 (mp-19087) 0.4957 0.000 4
CuS (mp-558139) 0.4112 0.286 2
FeO (mp-849689) 0.4487 0.104 2
MoN (mp-2811) 0.4152 0.000 2
SrO (mp-754282) 0.4532 0.090 2
TiS (mp-557762) 0.4254 0.139 2
Na6MnNi3(SbO6)2 (mp-1094109) 0.4858 0.139 5
Na (mp-999501) 0.4890 0.114 1
Te (mp-570459) 0.7374 0.044 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Na_pv Ti_pv S
Final Energy/Atom
-5.7117 eV
Corrected Energy
-24.1738 eV
-24.1738 eV = -22.8468 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)