Final Magnetic Moment0.703 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.942 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.065 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.22 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiAgF4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2/m [10] |
Hall-P 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 1 1> | 127.2 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 129.5 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 128.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 1> | 222.6 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 159.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 96.7 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 64.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 209.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 177.2 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 151.2 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 188.6 |
CeO2 (mp-20194) | <1 1 0> | <1 1 1> | 127.2 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 254.4 |
GaAs (mp-2534) | <1 1 0> | <1 1 1> | 95.4 |
GaAs (mp-2534) | <1 1 1> | <1 0 1> | 280.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 273.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 193.3 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 172.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 96.7 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 151.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 209.5 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 210.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 177.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 326.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 134.7 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 188.6 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 259.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 140.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 128.9 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 172.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 188.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 259.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 273.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 188.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 323.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 1> | 95.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 215.6 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 210.0 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 186.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 273.9 |
ZnSe (mp-1190) | <1 1 0> | <1 1 1> | 95.4 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 280.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 95.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 273.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 188.6 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 134.7 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 86.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 367.2 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 257.8 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 95.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MgUO4 (mp-7858) | 0.2015 | 0.000 | 3 |
UCoO4 (mp-565596) | 0.2852 | 0.170 | 3 |
UCoO4 (mp-19089) | 0.2049 | 0.170 | 3 |
UMnO4 (mp-19173) | 0.2134 | 0.000 | 3 |
UMnO4 (mp-639978) | 0.2502 | 0.492 | 3 |
LiMn2OF5 (mp-764255) | 0.4144 | 0.215 | 4 |
AlMo(WO4)2 (mvc-685) | 0.3810 | 0.076 | 4 |
AlV(WO4)2 (mvc-704) | 0.4220 | 0.014 | 4 |
YMo(WO4)2 (mvc-742) | 0.4161 | 0.055 | 4 |
TaAl(WO4)2 (mvc-640) | 0.3866 | 0.088 | 4 |
HgF2 (mp-974603) | 0.3250 | 0.008 | 2 |
Rb2O (mp-755459) | 0.3830 | 0.018 | 2 |
Na2O (mp-755072) | 0.3980 | 0.036 | 2 |
NdO2 (mp-754317) | 0.3320 | 0.298 | 2 |
OsO2 (mp-996) | 0.3983 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ag F |
Final Energy/Atom-3.6789 eV |
Corrected Energy-22.0734 eV
-22.0734 eV = -22.0734 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)