Final Magnetic Moment11.984 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.661 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.044 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToEu2SeO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 78.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 202.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 31.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 155.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 280.7 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 209.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 31.2 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 280.7 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 199.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 187.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 249.5 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 211.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 311.8 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 144.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 78.0 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 141.3 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 144.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 171.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 171.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 149.8 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 217.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 31.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 211.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 62.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 296.3 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 289.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 249.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 78.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 78.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 31.2 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 280.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 140.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 209.3 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 280.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 218.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 374.2 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 202.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 311.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 15.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 155.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 233.9 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 211.9 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 233.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 249.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 140.3 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 261.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 202.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 343.0 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 261.6 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 280.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
U2SbN2 (mp-5268) | 0.0260 | 0.000 | 3 |
Dy2SeO2 (mp-769253) | 0.0540 | 0.042 | 3 |
Tm2SeO2 (mp-754475) | 0.0506 | 0.045 | 3 |
La2TeO2 (mp-4547) | 0.0479 | 0.000 | 3 |
Ce2BiO2 (mp-23003) | 0.0469 | 0.000 | 3 |
KLiZnS2 (mp-774907) | 0.2922 | 0.000 | 4 |
SrBiClO2 (mp-547244) | 0.4657 | 0.000 | 4 |
SrBiBrO2 (mp-552234) | 0.4685 | 0.000 | 4 |
KLiMnS2 (mp-753940) | 0.2320 | 0.000 | 4 |
BiPbClO2 (mp-23084) | 0.3163 | 0.000 | 4 |
Bi3O2 (mp-1022722) | 0.6964 | 0.125 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Eu Se O |
Final Energy/Atom-9.1751 eV |
Corrected Energy-47.2802 eV
-47.2802 eV = -45.8756 eV (uncorrected energy) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)