Final Magnetic Moment0.017 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.802 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.097 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.25 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2TeO4 + LiSbO3 + TeO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 -1> | 48.7 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 204.9 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 -1> | 146.2 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 -1> | 243.7 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 -1> | 243.7 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 204.9 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 157.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 118.9 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 52.5 |
AlN (mp-661) | <1 1 1> | <0 1 -1> | 194.9 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 122.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 89.2 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 204.9 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 163.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 89.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 118.9 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 136.0 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 209.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 297.4 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 89.2 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 148.7 |
SiO2 (mp-6930) | <1 1 1> | <1 1 -1> | 260.6 |
KCl (mp-23193) | <1 0 0> | <0 1 -1> | 243.7 |
KCl (mp-23193) | <1 1 0> | <0 1 -1> | 292.4 |
KCl (mp-23193) | <1 1 1> | <0 1 -1> | 146.2 |
BaF2 (mp-1029) | <1 0 0> | <1 1 -1> | 325.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 29.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 29.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 89.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 267.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 122.9 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 209.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 345.7 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 262.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 -1> | 325.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 267.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 297.4 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 89.2 |
ZnSe (mp-1190) | <1 1 1> | <0 1 -1> | 341.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 89.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 302.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 89.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 52.5 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 163.9 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 259.3 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 129.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 89.2 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 327.1 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 163.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 209.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3FeF6 (mp-777488) | 0.3682 | 0.203 | 3 |
Li2FeF5 (mp-776886) | 0.3496 | 0.026 | 3 |
ZnGeO3 (mp-1020631) | 0.3770 | 0.107 | 3 |
Na(CoO2)3 (mp-690518) | 0.3558 | 0.281 | 3 |
LiOsO3 (mp-1078358) | 0.3704 | 0.000 | 3 |
Li4Nb(TeO4)3 (mp-759998) | 0.1633 | 0.088 | 4 |
Li2FeWO6 (mp-776913) | 0.2248 | 0.086 | 4 |
TiZn2WO6 (mvc-5957) | 0.1684 | 0.134 | 4 |
Zn2CoWO6 (mvc-6162) | 0.2174 | 0.057 | 4 |
Zn2MoWO6 (mvc-6039) | 0.2070 | 0.098 | 4 |
Pb2O3 (mp-20078) | 0.4599 | 0.009 | 2 |
Te2Ir (mp-569388) | 0.4699 | 0.000 | 2 |
V3O5 (mp-542441) | 0.4788 | 0.029 | 2 |
Mn5O8 (mp-18922) | 0.4050 | 0.009 | 2 |
Mn5O8 (mp-715008) | 0.3977 | 0.009 | 2 |
Li4MnSn(WO6)2 (mp-775961) | 0.1882 | 0.050 | 5 |
Li4MnCr(WO6)2 (mp-761370) | 0.2227 | 0.070 | 5 |
Li4ZrNb(TeO6)2 (mp-756177) | 0.2010 | 0.058 | 5 |
Li4VCr(TeO6)2 (mp-771088) | 0.2494 | 0.068 | 5 |
Li4TiMn(WO6)2 (mp-770980) | 0.1940 | 0.031 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Sb Te O |
Final Energy/Atom-5.4087 eV |
Corrected Energy-116.6016 eV
-116.6016 eV = -108.1742 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)