Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.990 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.46 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.073 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
Al (mp-134) | <1 1 0> | <1 1 0> | 0.000 | 254.0 |
Si (mp-149) | <1 1 0> | <1 1 0> | 0.000 | 84.7 |
Si (mp-149) | <1 0 0> | <1 0 0> | 0.000 | 59.9 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 0.000 | 84.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 0.000 | 59.9 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 0.000 | 299.3 |
BN (mp-984) | <0 0 1> | <1 1 1> | 0.000 | 103.7 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 0.001 | 179.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 0.001 | 299.3 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 0.004 | 239.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 0.004 | 254.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 0.006 | 299.3 |
TbScO3 (mp-31119) | <0 0 1> | <1 1 0> | 0.013 | 254.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 0.013 | 299.3 |
BN (mp-984) | <1 0 0> | <1 1 0> | 0.014 | 254.0 |
BN (mp-984) | <1 1 0> | <1 1 0> | 0.016 | 169.3 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 0.017 | 254.0 |
NdGaO3 (mp-3196) | <0 1 0> | <1 1 0> | 0.020 | 84.7 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 0.021 | 169.3 |
TiO2 (mp-2657) | <1 0 1> | <1 1 0> | 0.023 | 254.0 |
Au (mp-81) | <1 0 0> | <1 0 0> | 0.026 | 299.3 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 0.029 | 84.7 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 0.031 | 59.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 0.033 | 254.0 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 0.046 | 254.0 |
CaF2 (mp-2741) | <1 1 0> | <1 1 0> | 0.048 | 84.7 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 0.050 | 239.5 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 0.050 | 169.3 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 0.050 | 59.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 0.052 | 299.3 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 0.053 | 119.7 |
NdGaO3 (mp-3196) | <0 1 1> | <1 1 1> | 0.053 | 103.7 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 0.064 | 299.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 0.067 | 299.3 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 0.067 | 299.3 |
BN (mp-984) | <1 1 1> | <1 0 0> | 0.070 | 239.5 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 0.070 | 254.0 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 0.079 | 254.0 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 0.079 | 254.0 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 0.081 | 103.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 0.083 | 299.3 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 0.090 | 59.9 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 0.092 | 299.3 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 0.092 | 179.6 |
Al2O3 (mp-1143) | <1 0 0> | <1 1 0> | 0.092 | 254.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 0.097 | 299.3 |
SiC (mp-8062) | <1 1 1> | <1 0 0> | 0.097 | 299.3 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 0.097 | 299.3 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 0.097 | 179.6 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 0.098 | 299.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.95 | 0.00 | 0.00 |
0.00 | 2.95 | -0.00 |
0.00 | -0.00 | 2.95 |
Dielectric Tensor εij (total) |
||
---|---|---|
1501.91 | 0.00 | 0.00 |
0.00 | 1501.91 | -0.00 |
0.00 | -0.00 | 1501.91 |
Polycrystalline dielectric constant
εpoly∞
2.95
|
Polycrystalline dielectric constant
εpoly
1501.91
|
Refractive Index n1.72 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaTiF6 (mp-27315) | 0.2109 | 0.000 | 3 |
CaSnF6 (mp-8224) | 0.0135 | 0.000 | 3 |
CaZrF6 (mp-1025456) | 0.0636 | 0.000 | 3 |
CaPbF6 (mp-20463) | 0.1559 | 0.000 | 3 |
NaMoF6 (mp-600536) | 0.2039 | 0.000 | 3 |
CoAg3(CN)6 (mp-6573) | 0.6409 | 0.236 | 4 |
ErCo(CN)6 (mp-6185) | 0.5885 | 0.034 | 4 |
CdPd(CN)6 (mp-606650) | 0.5360 | 0.368 | 4 |
FeAg3(CN)6 (mp-568663) | 0.6877 | 0.307 | 4 |
WO3 (mp-715923) | 0.3165 | 0.002 | 2 |
TiF3 (mp-555601) | 0.3296 | 0.000 | 2 |
CoF3 (mp-603815) | 0.3204 | 0.005 | 2 |
SnF3 (mp-8289) | 0.1589 | 0.000 | 2 |
ScF3 (mp-559092) | 0.3302 | 0.002 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv F |
Final Energy/Atom-5.2192 eV |
Corrected Energy-43.4356 eV
-43.4356 eV = -41.7536 eV (uncorrected energy) - 1.6820 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)