Final Magnetic Moment1.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.265 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.177 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFeS + Li2S |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3 [147] |
Hall-P 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 171.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 300.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 138.8 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 171.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 214.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 300.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 277.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 300.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 138.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 343.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 208.3 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 208.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 214.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 208.3 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 69.4 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 214.7 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 244.9 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 244.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 343.5 |
Al (mp-134) | <1 1 0> | <1 0 0> | 69.4 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 300.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 171.7 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 240.5 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 0> | 208.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 214.7 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 127.7 |
C (mp-66) | <1 1 1> | <0 0 1> | 300.5 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 214.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 171.7 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 300.5 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 208.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 277.7 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 208.3 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 0 0> | 208.3 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 208.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 171.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 69.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 300.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 343.5 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 69.4 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 214.7 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 208.3 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 277.7 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 277.7 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 277.7 |
Ni (mp-23) | <1 0 0> | <1 0 1> | 244.9 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 300.5 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 208.3 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 300.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 42.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na14Cd2O9 (mp-27559) | 0.3837 | 0.000 | 3 |
Li14Mn2S9 (mp-756198) | 0.1294 | 0.000 | 3 |
Ce6Y2O15 (mp-758094) | 0.5280 | 0.016 | 3 |
Li14Co2S9 (mp-768268) | 0.1065 | 0.122 | 3 |
Ce4ThO9 (mp-753456) | 0.5209 | 0.075 | 3 |
Li14Cr2N8O (mp-542789) | 0.7165 | 0.169 | 4 |
Cu9S5 (mp-684710) | 0.4625 | 0.050 | 2 |
U6O11 (mp-761153) | 0.4076 | 0.043 | 2 |
Pr6O11 (mp-559771) | 0.4324 | 0.074 | 2 |
Ce5O9 (mp-32613) | 0.5125 | 0.007 | 2 |
Cu9Se5 (mp-673655) | 0.5036 | 0.080 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Fe_pv S |
Final Energy/Atom-4.2617 eV |
Corrected Energy-111.0697 eV
Uncorrected energy = -106.5427 eV
Composition-based energy adjustment (-0.503 eV/atom x 9.0 atoms) = -4.5270 eV
Corrected energy = -111.0697 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)