Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.991 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.057 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.42 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToYBr3 + BaBr2 |
Band Gap3.675 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 102.5 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 -1> | 120.8 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 189.7 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 241.6 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 166.4 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 178.8 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 166.4 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 120.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 243.3 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 102.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 241.6 |
TePb (mp-19717) | <1 1 0> | <1 0 -1> | 120.8 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 1> | 189.7 |
CdTe (mp-406) | <1 1 0> | <1 0 -1> | 120.8 |
SiC (mp-7631) | <1 1 0> | <1 0 -1> | 241.6 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 1> | 189.7 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 102.5 |
C (mp-66) | <1 0 0> | <0 1 1> | 178.8 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 166.4 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 262.2 |
InSb (mp-20012) | <1 1 0> | <1 0 -1> | 120.8 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 204.9 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 102.5 |
SiC (mp-11714) | <1 0 0> | <1 0 1> | 189.7 |
ZrO2 (mp-2858) | <0 1 0> | <1 1 0> | 166.4 |
Si (mp-149) | <1 1 0> | <1 1 0> | 166.4 |
YAlO3 (mp-3792) | <0 1 1> | <1 0 1> | 189.7 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 102.5 |
YAlO3 (mp-3792) | <1 1 1> | <1 0 1> | 189.7 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 121.6 |
SiC (mp-8062) | <1 1 0> | <1 0 -1> | 241.6 |
CsI (mp-614603) | <1 1 0> | <0 1 0> | 262.2 |
MgF2 (mp-1249) | <1 1 1> | <1 0 -1> | 120.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaFeF5 (mvc-14316) | 0.2267 | 0.000 | 3 |
CaVF5 (mvc-14225) | 0.2223 | 0.000 | 3 |
CaCrF5 (mvc-14169) | 0.2614 | 0.000 | 3 |
BaYCl5 (mp-755083) | 0.1024 | 0.042 | 3 |
BaYI5 (mp-754144) | 0.0815 | 0.076 | 3 |
U3O8 (mp-698) | 0.7260 | 0.003 | 2 |
U2O5 (mp-647814) | 0.6599 | 0.017 | 2 |
W3O8 (mp-715557) | 0.7387 | 0.006 | 2 |
Np2O5 (mp-554714) | 0.6478 | 0.000 | 2 |
U3O8 (mp-560402) | 0.6379 | 0.005 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Y_sv Br |
Final Energy/Atom-4.3583 eV |
Corrected Energy-61.0160 eV
-61.0160 eV = -61.0160 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)