Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.389 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.263 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmmm [65] |
Hall-C 2 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 294.2 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 245.9 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 278.2 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 147.2 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 227.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 82.0 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 278.2 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 328.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 211.1 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 151.7 |
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 149.5 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 163.9 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 75.9 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 257.3 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 177.0 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 177.0 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 245.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 227.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 278.2 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 149.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 177.0 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 163.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 210.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 278.2 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 126.4 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 168.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 126.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 294.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 257.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 224.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 171.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 303.4 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 163.9 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 257.3 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 257.3 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 278.2 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 210.2 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 328.7 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 224.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 224.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 294.2 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 227.6 |
Te2W (mp-22693) | <1 0 1> | <0 1 0> | 101.1 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 177.0 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 163.9 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 101.1 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 140.7 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 202.3 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 126.4 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 126.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
W5O12F (mp-767560) | 0.4842 | 0.066 | 3 |
Sb3O7F (mp-753495) | 0.1577 | 0.040 | 3 |
Nb3O7F (mp-753459) | 0.0096 | 0.028 | 3 |
Nb5O12F (mp-759636) | 0.6075 | 0.043 | 3 |
W3O7F (mp-765184) | 0.3362 | 0.026 | 3 |
U3O8 (mp-698) | 0.3363 | 0.003 | 2 |
W3O8 (mp-715557) | 0.4660 | 0.004 | 2 |
W3O8 (mp-19066) | 0.4637 | 0.024 | 2 |
W3O8 (mp-715582) | 0.4756 | 0.024 | 2 |
U3O8 (mp-560402) | 0.4026 | 0.012 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ta_pv O F |
Final Energy/Atom-9.4535 eV |
Corrected Energy-108.9040 eV
-108.9040 eV = -103.9880 eV (uncorrected energy) - 4.9160 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)