Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.692 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.028 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaI2 + BaI2 |
Band Gap3.817 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2/c [13] |
Hall-P 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 328.6 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 173.9 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 197.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 268.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 67.0 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 328.6 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 286.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 134.1 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 208.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 268.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 268.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 134.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 328.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 286.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 67.0 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 328.6 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 286.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 277.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 328.6 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 286.9 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 260.8 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 268.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 67.0 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 328.6 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 286.9 |
Te2W (mp-22693) | <0 1 1> | <1 0 -1> | 173.9 |
YVO4 (mp-19133) | <1 1 0> | <1 0 -1> | 260.8 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 328.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 69.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 201.1 |
GaSe (mp-1943) | <1 0 1> | <1 1 -1> | 218.0 |
BN (mp-984) | <1 0 1> | <0 0 1> | 201.1 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 131.4 |
Al (mp-134) | <1 0 0> | <1 0 0> | 277.8 |
Al (mp-134) | <1 1 0> | <0 1 0> | 328.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 -1> | 86.9 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 134.1 |
TeO2 (mp-2125) | <0 1 0> | <1 0 1> | 210.5 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 201.1 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 69.5 |
Fe3O4 (mp-19306) | <1 1 0> | <0 0 1> | 201.1 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 201.1 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 277.8 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 328.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 268.1 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 134.1 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 328.6 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 0> | 286.9 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 131.4 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 65.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HoTaO4 (mp-5985) | 0.5454 | 0.000 | 3 |
CeHfO4 (mp-752669) | 0.4974 | 0.056 | 3 |
BaCaI4 (mp-766348) | 0.4732 | 0.061 | 3 |
ErTaO4 (mp-3444) | 0.5464 | 0.000 | 3 |
PrBiO4 (mp-770111) | 0.5238 | 0.015 | 3 |
KNd(WO4)2 (mp-566034) | 0.7348 | 0.000 | 4 |
YSb(WO4)2 (mvc-675) | 0.5561 | 0.039 | 4 |
YBi(WO4)2 (mvc-679) | 0.6954 | 0.018 | 4 |
YSn(WO4)2 (mvc-705) | 0.6702 | 0.089 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Ca_sv I |
Final Energy/Atom-3.3625 eV |
Corrected Energy-40.3497 eV
-40.3497 eV = -40.3497 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)