Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.325 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.087 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPb3O4 + PbO2 |
Band Gap0.538 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmn21 [31] |
HallP 2ac 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 100.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 302.5 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 190.2 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 108.9 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 201.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.7 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 235.2 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 238.8 |
GaAs (mp-2534) | <1 1 1> | <1 0 1> | 237.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 165.0 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 47.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 309.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 165.0 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 238.8 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 291.9 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 185.7 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 238.8 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 299.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 142.6 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 268.8 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 185.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 185.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 165.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 330.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 226.8 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 318.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 61.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 268.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 165.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 128.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 226.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 47.5 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 237.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 47.5 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 106.1 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 50.4 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 214.2 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 201.6 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 237.7 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 47.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 226.8 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 212.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 67.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 165.0 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 288.7 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 134.4 |
YVO4 (mp-19133) | <1 1 1> | <1 1 1> | 163.3 |
Te2W (mp-22693) | <0 1 1> | <0 1 1> | 235.2 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 53.1 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 67.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
-1.38690 | -0.61616 | -0.54127 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.51240 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.87072 | 0.00000 |
Piezoelectric Modulus ‖eij‖max1.61125 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
8.70 | 0.00 | 0.00 |
0.00 | 12.13 | 0.00 |
0.00 | 0.00 | 10.71 |
Dielectric Tensor εij (total) |
||
---|---|---|
36.98 | 0.00 | 0.00 |
0.00 | 28.47 | 0.00 |
0.00 | 0.00 | 73.36 |
Polycrystalline dielectric constant
εpoly∞
10.51
|
Polycrystalline dielectric constant
εpoly
46.27
|
Refractive Index n3.24 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YZr4O9 (mp-758784) | 0.6781 | 0.068 | 3 |
VOF (mp-767367) | 0.6624 | 0.220 | 3 |
CeZr11O24 (mp-752706) | 0.6943 | 0.017 | 3 |
VOF (mp-764286) | 0.4934 | 0.030 | 3 |
VOF (mp-768037) | 0.6982 | 0.012 | 3 |
EuI2 (mp-23305) | 0.6550 | 0.013 | 2 |
SrBr2 (mp-567744) | 0.6778 | 0.000 | 2 |
SrI2 (mp-568284) | 0.6102 | 0.000 | 2 |
EuI2 (mp-570799) | 0.7245 | 0.018 | 2 |
CeSe2 (mp-1080853) | 0.7315 | 0.029 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pb_d O |
Final Energy/Atom-5.3572 eV |
Corrected Energy-57.7862 eV
-57.7862 eV = -53.5725 eV (uncorrected energy) - 4.2137 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)