Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.010 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.013 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.05 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSn4P3 + P |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 337.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 337.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 241.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 241.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 337.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 144.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 241.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 193.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 281.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 241.3 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 161.1 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 161.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 337.8 |
BN (mp-984) | <0 0 1> | <1 1 1> | 147.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 193.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 337.8 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 241.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 139.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 193.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 337.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 241.6 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 161.1 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 241.3 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 337.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 337.8 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 337.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 193.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 193.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 193.0 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 0 0> | 161.1 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 193.0 |
C (mp-66) | <1 1 0> | <1 0 0> | 161.1 |
C (mp-66) | <1 1 1> | <0 0 1> | 193.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 337.8 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 241.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 144.8 |
MoS2 (mp-1434) | <0 0 1> | <1 0 1> | 281.6 |
MoS2 (mp-1434) | <1 0 0> | <1 0 1> | 281.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 193.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 337.8 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 139.5 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 337.8 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 241.3 |
Mg (mp-153) | <0 0 1> | <1 0 1> | 281.6 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 337.8 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 241.6 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 1 0> | 139.5 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 1 0> | 139.5 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 48.3 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 161.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
101 | 28 | 29 | 14 | 0 | 0 |
28 | 101 | 29 | -14 | 0 | 0 |
29 | 29 | 43 | 0 | 0 | 0 |
14 | -14 | 0 | 27 | 0 | 0 |
0 | 0 | 0 | 0 | 27 | 14 |
0 | 0 | 0 | 0 | 14 | 37 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
14 | -2.9 | -7.5 | -8.7 | 0 | 0 |
-2.9 | 14 | -7.5 | 8.7 | 0 | 0 |
-7.5 | -7.5 | 33.5 | 0 | 0 | 0 |
-8.7 | 8.7 | 0 | 45.4 | 0 | 0 |
0 | 0 | 0 | 0 | 45.4 | -17.4 |
0 | 0 | 0 | 0 | -17.4 | 33.9 |
Shear Modulus GV29 GPa |
Bulk Modulus KV46 GPa |
Shear Modulus GR22 GPa |
Bulk Modulus KR39 GPa |
Shear Modulus GVRH25 GPa |
Bulk Modulus KVRH43 GPa |
Elastic Anisotropy1.87 |
Poisson's Ratio0.25 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na13Ni11O24 (mp-768107) | 0.6547 | 0.021 | 3 |
Na2CoO3 (mp-779078) | 0.6587 | 0.114 | 3 |
Na2VO3 (mp-764060) | 0.6490 | 0.071 | 3 |
Na2CoO3 (mp-773768) | 0.6571 | 0.123 | 3 |
Na2VO3 (mp-780913) | 0.6521 | 0.184 | 3 |
K3NaTh2O6 (mp-17850) | 0.7279 | 0.000 | 4 |
AgSbPbS3 (mp-605863) | 0.6718 | 0.048 | 4 |
GeP3 (mp-7542) | 0.3759 | 0.028 | 2 |
InP3 (mp-20050) | 0.2752 | 0.053 | 2 |
Te2Au (mp-20123) | 0.6672 | 0.000 | 2 |
Te2Au (mp-571547) | 0.5546 | 0.010 | 2 |
Bi4I (mp-583234) | 0.7154 | 0.040 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sn_d P |
Final Energy/Atom-5.0677 eV |
Corrected Energy-40.5418 eV
-40.5418 eV = -40.5418 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)