Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.768 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.048 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBi2O3 + Y2O3 |
Band Gap2.603 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 220.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 220.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 126.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 220.6 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 275.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 220.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 183.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 252.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 283.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 283.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 220.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 189.1 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 158.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 220.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 283.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 252.2 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 158.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 157.6 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 220.6 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 158.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 283.7 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 91.8 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 94.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 157.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 126.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 31.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 126.1 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 275.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 283.7 |
BN (mp-984) | <1 0 0> | <1 0 0> | 275.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 220.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 94.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 283.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 220.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 283.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 346.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 346.7 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 220.6 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 220.6 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 91.8 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 157.6 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 94.6 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 283.7 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 126.1 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 346.7 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 126.1 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 31.5 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 220.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 157.6 |
C (mp-66) | <1 1 1> | <0 0 1> | 283.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TmBiO3 (mp-755216) | 0.1157 | 0.054 | 3 |
LuBiO3 (mp-772801) | 0.1943 | 0.059 | 3 |
ErBiO3 (mp-754636) | 0.0752 | 0.052 | 3 |
HoBiO3 (mp-754300) | 0.0582 | 0.050 | 3 |
TmBiO3 (mp-754323) | 0.2362 | 0.030 | 3 |
Li3Nb4NiO12 (mp-772009) | 0.4044 | 0.089 | 4 |
Li3Nb4FeO12 (mp-771984) | 0.4316 | 0.039 | 4 |
TiFe(BiO3)2 (mp-560185) | 0.4323 | 0.015 | 4 |
Mg2VWO6 (mvc-5881) | 0.4409 | 0.023 | 4 |
InNi2SbO6 (mp-1078367) | 0.3764 | 0.000 | 4 |
Y2O3 (mp-775906) | 0.2919 | 0.063 | 2 |
Y2O3 (mp-754759) | 0.3081 | 0.051 | 2 |
Fe2O3 (mp-542309) | 0.3323 | 0.131 | 2 |
Al2O3 (mp-1938) | 0.3202 | 0.093 | 2 |
In2O3 (mp-22323) | 0.3225 | 0.029 | 2 |
Li4Fe2TeWO12 (mp-768021) | 0.6199 | 0.083 | 5 |
Li4Cr2TeWO12 (mp-775566) | 0.7177 | 0.080 | 5 |
Li4Mn2TeWO12 (mp-768044) | 0.6882 | 0.058 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv Bi O |
Final Energy/Atom-7.3865 eV |
Corrected Energy-78.0790 eV
-78.0790 eV = -73.8653 eV (uncorrected energy) - 4.2137 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)