Final Magnetic Moment0.343 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.453 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.070 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.79 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2ZrO3 + CuO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4m2 [119] |
HallI 4 2 |
Point Group42m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaTe (mp-542812) | <0 0 1> | <1 0 0> | 76.2 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 342.9 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 152.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 214.8 |
CaF2 (mp-2741) | <1 1 0> | <1 0 0> | 342.9 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 1> | 84.2 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 71.6 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 161.1 |
ZnO (mp-2133) | <1 0 0> | <1 0 1> | 210.4 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 161.1 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 143.2 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 35.8 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 196.9 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 210.4 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 304.8 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 266.7 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 283.8 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 35.8 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 76.2 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 152.4 |
Si (mp-149) | <1 1 0> | <1 0 0> | 342.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 342.9 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 340.0 |
C (mp-48) | <0 0 1> | <1 0 1> | 42.1 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 114.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 340.6 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 1> | 336.7 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 71.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 342.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 286.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 17.9 |
Al (mp-134) | <1 1 0> | <1 0 1> | 210.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 196.9 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 190.5 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 268.4 |
BN (mp-984) | <1 0 0> | <1 1 0> | 215.5 |
YAlO3 (mp-3792) | <0 1 1> | <1 0 0> | 190.5 |
Bi2Se3 (mp-541837) | <1 0 0> | <0 0 1> | 125.3 |
Ga2O3 (mp-886) | <1 1 -1> | <0 0 1> | 161.1 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 214.8 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 89.5 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 304.2 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 126.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 161.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 210.4 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 89.5 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 232.6 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 71.6 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 0 1> | 232.6 |
PbS (mp-21276) | <1 1 1> | <1 0 0> | 304.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
279 | 88 | 88 | 0 | 0 | 0 |
88 | 279 | 88 | 0 | 0 | 0 |
88 | 88 | 92 | 0 | 0 | 0 |
0 | 0 | 0 | 70 | 0 | 0 |
0 | 0 | 0 | 0 | 70 | 0 |
0 | 0 | 0 | 0 | 0 | 98 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
5.1 | -0.1 | -4.8 | 0 | 0 | 0 |
-0.1 | 5.1 | -4.8 | 0 | 0 | 0 |
-4.8 | -4.8 | 20.2 | 0 | 0 | 0 |
0 | 0 | 0 | 14.2 | 0 | 0 |
0 | 0 | 0 | 0 | 14.2 | 0 |
0 | 0 | 0 | 0 | 0 | 10.2 |
Shear Modulus GV73 GPa |
Bulk Modulus KV131 GPa |
Shear Modulus GR54 GPa |
Bulk Modulus KR92 GPa |
Shear Modulus GVRH64 GPa |
Bulk Modulus KVRH111 GPa |
Elastic Anisotropy2.20 |
Poisson's Ratio0.26 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YAgSe2 (mp-676284) | 0.1753 | 0.041 | 3 |
NaNdS2 (mp-676360) | 0.1558 | 0.012 | 3 |
NaLaS2 (mp-675230) | 0.1677 | 0.002 | 3 |
NaPrS2 (mp-675199) | 0.1710 | 0.009 | 3 |
NaCeS2 (mp-36536) | 0.1643 | 0.025 | 3 |
Li2CuBiO4 (mp-754238) | 0.0643 | 0.112 | 4 |
LiTe3 (mp-27466) | 0.2507 | 0.009 | 2 |
CoO (mp-561809) | 0.4341 | 0.037 | 2 |
CdTe (mp-12581) | 0.4492 | 0.486 | 2 |
SrN (mp-1078609) | 0.4397 | 0.438 | 2 |
Sb2Te3 (mp-1080789) | 0.3415 | 0.128 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.7441 | 0.005 | 5 |
Hg (mp-982872) | 0.4851 | 0.020 | 1 |
Se (mp-7755) | 0.5097 | 0.181 | 1 |
Te (mp-10654) | 0.5164 | 0.047 | 1 |
Te (mp-105) | 0.4103 | 0.047 | 1 |
P (mp-53) | 0.5162 | 0.144 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Zr_sv Cu_pv O |
Final Energy/Atom-6.6344 eV |
Corrected Energy-55.8845 eV
-55.8845 eV = -53.0753 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)