Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.271 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.022 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.98 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToKSnPO5 + K3PO4 + SnO2 + K2CO3 + C |
Band Gap3.481 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 0> | 287.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 288.5 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 288.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 300.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 300.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 300.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 128.9 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 173.1 |
GaSe (mp-1943) | <1 0 1> | <1 1 1> | 212.3 |
BN (mp-984) | <1 0 0> | <1 0 0> | 76.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 257.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 128.9 |
BN (mp-984) | <1 1 1> | <0 1 0> | 230.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 214.8 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 287.8 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 212.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 214.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 300.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 214.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 128.9 |
Al (mp-134) | <1 1 1> | <1 0 0> | 229.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 214.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 214.8 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 287.8 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 1> | 287.8 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 214.8 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 300.7 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 214.8 |
SiC (mp-7631) | <0 0 1> | <1 1 0> | 191.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 128.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 128.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 257.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 229.9 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 257.8 |
Fe3O4 (mp-19306) | <1 0 0> | <1 1 1> | 212.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 214.8 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 76.6 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 343.7 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 267.3 |
TiO2 (mp-2657) | <1 0 0> | <1 0 1> | 178.2 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 128.9 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 214.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 214.8 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 229.9 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 214.8 |
C (mp-66) | <1 0 0> | <0 0 1> | 343.7 |
C (mp-66) | <1 1 0> | <0 1 0> | 230.8 |
C (mp-66) | <1 1 1> | <0 1 1> | 287.8 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 230.8 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 128.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3CaPCO7 (mp-767552) | 0.2692 | 0.000 | 5 |
K3CaPCO7 (mp-756968) | 0.2306 | 0.000 | 5 |
K3GePCO7 (mp-756801) | 0.2534 | 0.062 | 5 |
K3SrPCO7 (mp-772777) | 0.1362 | 0.011 | 5 |
Na3GePCO7 (mp-768125) | 0.2659 | 0.065 | 5 |
Na5LiMn2P2(CO7)2 (mp-773420) | 0.2577 | 0.016 | 6 |
Na5LiMn2P2(CO7)2 (mp-773413) | 0.2694 | 0.209 | 6 |
Na5LiMn2P2(CO7)2 (mp-770027) | 0.2559 | 0.011 | 6 |
Na5LiMn2P2(CO7)2 (mp-773941) | 0.2682 | 0.014 | 6 |
Na5LiMn2P2(CO7)2 (mp-773680) | 0.2829 | 0.208 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Sn_d P C O |
Final Energy/Atom-6.2480 eV |
Corrected Energy-172.2799 eV
-172.2799 eV = -162.4478 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)