Final Magnetic Moment2.297 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.387 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.129 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi4TeO5 + Li2TeO3 + CuO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 1> | 290.0 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 203.3 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 304.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 193.1 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 255.8 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 257.5 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 193.1 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 213.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 254.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 321.9 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 290.0 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 341.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 170.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 213.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 255.8 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 304.9 |
CdS (mp-672) | <1 0 1> | <1 1 -1> | 289.4 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 247.4 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 213.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 85.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 255.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 203.3 |
Te2W (mp-22693) | <1 0 0> | <1 0 -1> | 101.6 |
Te2W (mp-22693) | <1 0 1> | <1 0 -1> | 101.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 213.1 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 321.9 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 64.4 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 42.6 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 298.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 341.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 321.9 |
Te2Mo (mp-602) | <1 1 1> | <1 1 -1> | 289.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 85.3 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 247.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 -1> | 289.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 -1> | 50.8 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 257.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 254.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 170.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 341.0 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 213.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 257.5 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 152.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 42.6 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 290.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 -1> | 217.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 254.1 |
BN (mp-984) | <0 0 1> | <1 0 -1> | 152.4 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 254.1 |
BN (mp-984) | <1 0 1> | <1 0 -1> | 254.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CdAgO2 (mp-996963) | 0.6326 | 0.024 | 3 |
NaCu2O3 (mp-779328) | 0.5948 | 0.100 | 3 |
NaCu3O4 (mp-773466) | 0.7339 | 0.097 | 3 |
Li5Cu5(SnO6)2 (mp-770470) | 0.7060 | 0.088 | 4 |
Li5Cu3(NiO5)2 (mp-773166) | 0.7208 | 0.082 | 4 |
Li4Cu3WO8 (mp-771990) | 0.6376 | 0.136 | 4 |
Na3Cu2SbO6 (mp-12860) | 0.6961 | 0.056 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv Te O |
Final Energy/Atom-5.0893 eV |
Corrected Energy-87.0474 eV
-87.0474 eV = -81.4291 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)