Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.004 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.113 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBaO2 + BaNd2O4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3c [167] |
Hall-R 3 2"c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 326.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 254.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 254.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 181.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 108.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 326.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 181.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 200.5 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 290.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 36.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 100.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 362.9 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 173.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 145.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 290.4 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 173.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 181.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 1> | 177.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 181.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 254.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 254.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 181.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 108.9 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 100.3 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 100.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 254.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 181.5 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 200.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 108.9 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 326.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 254.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 200.5 |
BN (mp-984) | <0 0 1> | <1 0 1> | 213.3 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 213.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 145.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 326.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 326.6 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 100.3 |
BN (mp-984) | <1 0 0> | <1 0 1> | 213.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 108.9 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 145.2 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 213.3 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 108.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 254.1 |
Al (mp-134) | <1 1 0> | <0 0 1> | 181.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 108.9 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 100.3 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 254.1 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 254.1 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 254.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaPrO3 (mp-6910) | 0.1192 | 0.115 | 3 |
TbNiO3 (mp-770347) | 0.1803 | 0.042 | 3 |
LuAlO3 (mp-754435) | 0.1169 | 0.082 | 3 |
PrTiO3 (mp-753948) | 0.1585 | 0.059 | 3 |
LaFeO3 (mp-1078634) | 0.1301 | 0.000 | 3 |
La2ZnMoO6 (mvc-11208) | 0.1915 | 0.052 | 4 |
La2MgWO6 (mvc-15459) | 0.1343 | 0.133 | 4 |
La2ZnSnO6 (mvc-15177) | 0.1965 | 0.078 | 4 |
La2MgSnO6 (mvc-13582) | 0.1505 | 0.033 | 4 |
In2Ag (mp-760385) | 0.6476 | 0.096 | 2 |
SiO2 (mp-10948) | 0.7498 | 0.254 | 2 |
Hf2Ge (mp-1072256) | 0.6545 | 0.622 | 2 |
CaLa9Ti5Cr5O30 (mp-694926) | 0.3930 | 0.063 | 5 |
Ca2La8Ti5Cr5O30 (mp-743953) | 0.3860 | 0.046 | 5 |
SrLa7TiGa7O24 (mp-720505) | 0.4701 | 0.015 | 5 |
SrLaMnRuO6 (mp-39239) | 0.3803 | 0.094 | 5 |
SrLaMnRuO6 (mp-690590) | 0.3418 | 0.094 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Nd_3 O |
Final Energy/Atom-6.8886 eV |
Corrected Energy-73.0995 eV
-73.0995 eV = -68.8858 eV (uncorrected energy) - 4.2137 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)