material

Y2CuO4

ID:

mp-754364

DOI:

10.17188/1289398


Material Details

Final Magnetic Moment
0.006 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.055 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.051 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.71 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Y2O3 + CuO
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GdScO3 (mp-5690) <1 1 1> <0 0 1> 0.020 286.7
GaP (mp-2490) <1 0 0> <0 0 1> 0.020 30.2
Mg (mp-153) <0 0 1> <0 0 1> 0.026 166.0
SiO2 (mp-6930) <1 0 0> <1 1 0> 0.028 194.0
C (mp-48) <1 0 0> <1 0 1> 0.031 96.3
GdScO3 (mp-5690) <1 0 1> <0 0 1> 0.038 226.3
Mg (mp-153) <1 1 0> <1 1 0> 0.039 258.6
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.044 196.1
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.046 135.8
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.047 129.3
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.053 120.7
GaP (mp-2490) <1 1 0> <1 1 0> 0.055 129.3
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.061 30.2
Te2W (mp-22693) <0 0 1> <0 0 1> 0.062 331.9
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.063 129.3
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.063 166.0
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.066 256.5
Ga2O3 (mp-886) <1 0 -1> <1 0 1> 0.069 192.6
Si (mp-149) <1 0 0> <0 0 1> 0.070 30.2
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.077 30.2
MgO (mp-1265) <1 1 0> <0 0 1> 0.081 331.9
Ga2O3 (mp-886) <1 0 0> <1 0 1> 0.083 144.4
CaCO3 (mp-3953) <1 1 0> <0 0 1> 0.085 150.9
TbScO3 (mp-31119) <1 1 1> <0 0 1> 0.099 286.7
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.107 196.1
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.109 194.0
SiC (mp-7631) <1 0 1> <0 0 1> 0.122 241.4
Ni (mp-23) <1 1 0> <1 1 0> 0.135 194.0
Ag (mp-124) <1 1 0> <1 1 0> 0.138 194.0
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.141 316.8
TiO2 (mp-2657) <1 0 1> <1 1 0> 0.143 129.3
BaF2 (mp-1029) <1 1 0> <1 1 1> 0.146 332.0
InAs (mp-20305) <1 0 0> <0 0 1> 0.149 75.4
TbScO3 (mp-31119) <1 0 1> <0 0 1> 0.160 226.3
NdGaO3 (mp-3196) <1 1 0> <0 0 1> 0.168 60.4
AlN (mp-661) <1 0 0> <0 0 1> 0.170 316.8
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.175 75.4
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.186 286.7
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.192 316.8
Te2W (mp-22693) <0 1 0> <0 0 1> 0.196 271.6
PbSe (mp-2201) <1 1 0> <1 1 1> 0.201 332.0
CsI (mp-614603) <1 1 0> <1 1 0> 0.204 258.6
DyScO3 (mp-31120) <1 1 1> <0 0 1> 0.204 286.7
SiO2 (mp-6930) <1 1 0> <1 1 0> 0.208 194.0
LiGaO2 (mp-5854) <1 1 1> <1 1 1> 0.208 332.0
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.212 286.7
C (mp-48) <1 1 1> <0 0 1> 0.221 301.8
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.226 135.8
Al (mp-134) <1 1 0> <0 0 1> 0.236 256.5
Au (mp-81) <1 1 0> <1 1 0> 0.239 194.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
284 162 51 0 0 0
162 284 51 0 0 0
51 51 242 0 0 0
0 0 0 25 0 0
0 0 0 0 25 0
0 0 0 0 0 133
Compliance Tensor Sij (10-12Pa-1)
5.3 -2.9 -0.5 0 0 0
-2.9 5.3 -0.5 0 0 0
-0.5 -0.5 4.3 0 0 0
0 0 0 40.3 0 0
0 0 0 0 40.3 0
0 0 0 0 0 7.5
Shear Modulus GV
73 GPa
Bulk Modulus KV
149 GPa
Shear Modulus GR
44 GPa
Bulk Modulus KR
142 GPa
Shear Modulus GVRH
59 GPa
Bulk Modulus KVRH
145 GPa
Elastic Anisotropy
3.31
Poisson's Ratio
0.32

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
La2PdO4 (mp-8672) 0.0506 0.055 3
In2CuO4 (mp-20476) 0.0824 0.248 3
Ho2CuO4 (mp-754327) 0.0065 0.050 3
Gd2CuO4 (mp-4860) 0.0464 0.000 3
Sm2CuO4 (mp-4210) 0.0580 0.008 3
Ba2Pd(OF)2 (mp-6123) 0.4947 0.052 4
LiNd14(Cu3O14)2 (mp-766561) 0.1497 0.009 4
LiNd6(CuO6)2 (mp-756531) 0.2354 0.026 4
LiLa4AuO8 (mp-560605) 0.0664 0.000 4
Ce2Cu(NO)2 (mp-1022723) 0.0422 0.274 4
Sr2Ti2Bi2OF2 (mp-1078216) 0.6829 0.000 5
Sr2Ti2Sb2OF2 (mp-1079717) 0.7284 0.000 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Cu_pv O
Final Energy/Atom
-7.9226 eV
Corrected Energy
-58.2062 eV
Uncorrected energy = -55.4582 eV Composition-based energy adjustment (-0.687 eV/atom x 4.0 atoms) = -2.7480 eV Corrected energy = -58.2062 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)