Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.747 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom< 0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.34 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBa3Tm4O9 + Tm2O3 |
Band Gap3.613 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 288.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 320.9 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 272.7 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 165.1 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 288.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 285.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 178.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 213.9 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 288.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 272.7 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 165.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 213.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 142.6 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 247.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 213.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 107.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 130.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 178.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 356.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 320.9 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 288.9 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 206.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 178.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 272.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 288.9 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 206.4 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 272.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 206.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 285.2 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 163.6 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 123.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 107.0 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 178.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 107.0 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 272.7 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 163.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 213.9 |
TePb (mp-19717) | <1 1 1> | <0 1 0> | 288.9 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 131.9 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 260.6 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 123.8 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 123.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 330.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 163.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 320.9 |
BN (mp-984) | <1 0 0> | <0 0 1> | 249.6 |
BN (mp-984) | <1 0 1> | <0 1 1> | 163.6 |
BN (mp-984) | <1 1 1> | <0 1 1> | 272.7 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 165.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 285.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaLu2O4 (mp-752442) | 0.0362 | 0.005 | 3 |
BaHo2O4 (mp-17363) | 0.0881 | 0.000 | 3 |
BaTb2O4 (mp-18258) | 0.1344 | 0.000 | 3 |
BaY2O4 (mp-3952) | 0.1290 | 0.000 | 3 |
BaGd2O4 (mp-17143) | 0.1643 | 0.000 | 3 |
Ca5Sc2(CoO6)2 (mvc-13126) | 0.7293 | 0.027 | 4 |
FeBiSbS4 (mp-601716) | 0.6840 | 0.170 | 4 |
Na3Mn4(TeO6)2 (mp-565229) | 0.5578 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Tm_3 O |
Final Energy/Atom-7.7256 eV |
Corrected Energy-227.5527 eV
-227.5527 eV = -216.3160 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)