material

Al2O3

ID:

mp-754624

DOI:

10.17188/1289493


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.361 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.065 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.68 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Al2O3
Band Gap
5.797 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3 [148]
Hall
-R 3
Point Group
3
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
InAs (mp-20305) <1 1 1> <0 0 1> 0.000 264.7
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.000 142.5
TeO2 (mp-2125) <0 1 1> <1 1 0> 0.000 227.7
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.001 264.7
C (mp-48) <0 0 1> <0 0 1> 0.001 142.5
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.004 264.7
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.005 183.2
C (mp-66) <1 1 1> <0 0 1> 0.009 264.7
CdS (mp-672) <0 0 1> <0 0 1> 0.010 61.1
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.011 61.1
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.021 142.5
Mg (mp-153) <0 0 1> <0 0 1> 0.029 61.1
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.030 183.2
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.031 183.2
InP (mp-20351) <1 1 1> <0 0 1> 0.031 61.1
TiO2 (mp-390) <1 1 0> <1 0 0> 0.054 263.0
SrTiO3 (mp-4651) <1 0 0> <1 0 0> 0.057 131.5
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.060 162.9
GaN (mp-804) <1 1 0> <1 0 0> 0.073 263.0
TiO2 (mp-2657) <1 0 1> <1 0 1> 0.073 206.5
CsI (mp-614603) <1 1 0> <1 0 0> 0.074 263.0
CdS (mp-672) <1 1 1> <1 0 1> 0.081 206.5
CdSe (mp-2691) <1 1 1> <0 0 1> 0.087 264.7
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.087 61.1
WS2 (mp-224) <0 0 1> <0 0 1> 0.088 61.1
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.093 264.7
CdS (mp-672) <1 0 0> <1 1 0> 0.096 113.9
CdS (mp-672) <1 1 0> <1 0 0> 0.096 197.2
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.108 101.8
LaF3 (mp-905) <1 1 0> <1 0 1> 0.120 275.3
Mg (mp-153) <1 1 0> <1 0 0> 0.122 263.0
GaSb (mp-1156) <1 1 1> <0 0 1> 0.124 264.7
WSe2 (mp-1821) <1 1 1> <0 0 1> 0.148 264.7
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.152 183.2
GaTe (mp-542812) <0 0 1> <0 0 1> 0.159 305.4
PbSe (mp-2201) <1 1 1> <0 0 1> 0.180 264.7
GaAs (mp-2534) <1 0 0> <0 0 1> 0.187 366.5
LiAlO2 (mp-3427) <1 0 0> <1 1 0> 0.211 227.7
GaTe (mp-542812) <1 0 -1> <0 0 1> 0.223 305.4
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.225 366.5
MgO (mp-1265) <1 1 0> <0 0 1> 0.233 101.8
InP (mp-20351) <1 1 0> <1 0 0> 0.237 197.2
AlN (mp-661) <1 0 1> <0 0 1> 0.254 264.7
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.263 20.4
LiF (mp-1138) <1 1 1> <0 0 1> 0.264 264.7
TiO2 (mp-390) <1 0 0> <1 0 0> 0.275 263.0
GaSe (mp-1943) <0 0 1> <0 0 1> 0.279 244.3
MgO (mp-1265) <1 0 0> <0 0 1> 0.286 142.5
CaF2 (mp-2741) <1 1 0> <1 0 0> 0.305 131.5
Ag (mp-124) <1 1 1> <0 0 1> 0.308 264.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
443 125 68 7 8 0
125 443 68 -7 -8 0
68 68 331 0 0 0
7 -7 0 89 0 -8
8 -8 0 0 89 7
0 0 0 -8 7 159
Compliance Tensor Sij (10-12Pa-1)
2.5 -0.7 -0.4 -0.2 -0.3 0
-0.7 2.5 -0.4 0.2 0.3 0
-0.4 -0.4 3.2 0 0 0
-0.2 0.2 0 11.3 0 0.6
-0.3 0.3 0 0 11.3 -0.5
0 0 0 0.6 -0.5 6.3
Shear Modulus GV
131 GPa
Bulk Modulus KV
193 GPa
Shear Modulus GR
120 GPa
Bulk Modulus KR
186 GPa
Shear Modulus GVRH
126 GPa
Bulk Modulus KVRH
190 GPa
Elastic Anisotropy
0.51
Poisson's Ratio
0.23

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li(FeO2)3 (mp-763849) 0.2877 0.128 3
Li(CoO2)3 (mp-763697) 0.2968 0.009 3
Na3YCl6 (mp-675104) 0.1927 0.000 3
Li3FeF6 (mp-777475) 0.1786 0.025 3
Na3GdCl6 (mp-33554) 0.2265 0.000 3
Li2Mn3(FeO4)3 (mp-767665) 0.2741 0.098 4
Li2Mn3Cr3O12 (mp-850956) 0.2648 0.075 4
Li2Ti3V3O12 (mp-763640) 0.2756 0.093 4
LiAl2FeO6 (mp-770071) 0.2694 0.134 4
LiV2CrO6 (mp-849360) 0.3287 0.106 4
Al2O3 (mp-755175) 0.1117 0.072 2
Cr2O3 (mp-776999) 0.3054 0.062 2
Ti2O3 (mp-776655) 0.3291 0.079 2
Sc2O3 (mp-754455) 0.2181 0.086 2
Cr2S3 (mp-13685) 0.3956 0.001 2
Li4V2Cr3Sb3O16 (mp-775451) 0.7465 0.098 5
Li4Fe3Co2Sn3O16 (mp-775387) 0.7234 0.111 5
Li4Fe2TeWO12 (mp-768021) 0.6104 0.085 5
Li4Cr2TeWO12 (mp-775566) 0.7211 0.080 5
Li4Mn2TeWO12 (mp-768044) 0.6753 0.058 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

A series of sulfated zirconia (SZ) were prepared by solgel methods, from Zrn-propoxide, either with thein situone-step addition of H2SO4during the gelification process, or byex situsulfation of a Zr( [...]
TiO2Al2O3 (TiAl) and Al2O3 (Al) supports were prepared according to a previously developed procedure (Galiasso Tailleur and Ravigli Nascar [20]). TiAl support is formed by co-precipitation of alkoxide [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition Al2O3.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Al O
Final Energy/Atom
-7.4159 eV
Corrected Energy
-78.2806 eV
Uncorrected energy = -74.1586 eV Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV Corrected energy = -78.2806 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)