Final Magnetic Moment7.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.538 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.321 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3 [147] |
Hall-P 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 105.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 316.5 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 272.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 124.7 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 291.0 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 216.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 175.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 175.8 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 249.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 166.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 281.3 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 166.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 35.2 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 207.9 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 272.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 175.8 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 240.4 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 166.3 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 326.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 332.6 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 216.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 332.6 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 41.6 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 281.3 |
TiO2 (mp-2657) | <0 0 1> | <1 1 0> | 216.0 |
TiO2 (mp-2657) | <1 0 1> | <1 0 1> | 326.7 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 207.9 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 291.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 246.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 175.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 216.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 316.5 |
C (mp-66) | <1 0 0> | <1 0 0> | 166.3 |
C (mp-66) | <1 1 0> | <1 0 0> | 166.3 |
C (mp-66) | <1 1 1> | <1 0 0> | 332.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 281.3 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 166.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 166.3 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 316.5 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 175.8 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 216.0 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 316.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 272.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 249.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 246.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 105.5 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 326.7 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 272.3 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 35.2 |
Mg (mp-153) | <1 0 0> | <1 0 1> | 163.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Er(ReO4)2 (mp-755194) | 0.2483 | 0.017 | 3 |
Pr(ReO4)2 (mp-754632) | 0.0837 | 0.000 | 3 |
Co(ClO4)2 (mp-31621) | 0.4429 | 0.000 | 3 |
Mg(ReO4)2 (mp-754311) | 0.3601 | 0.000 | 3 |
Bi2(SO4)3 (mp-768482) | 0.4523 | 0.011 | 3 |
ZrP2(HO3)2 (mp-24030) | 0.5316 | 0.000 | 4 |
ZrP2(HO3)2 (mp-643013) | 0.3664 | 0.003 | 4 |
Cs3Yb(SO4)3 (mp-558829) | 0.4764 | 0.000 | 4 |
MgPHO9 (mp-632723) | 0.5705 | 0.860 | 4 |
MgPHO9 (mp-720260) | 0.5714 | 0.859 | 4 |
Cr3O8 (mp-782705) | 0.6585 | 0.047 | 2 |
PCl5 (mp-23228) | 0.6972 | 0.000 | 2 |
Cr3O8 (mp-557959) | 0.7064 | 0.045 | 2 |
InPH5NO5 (mp-764968) | 0.5807 | 0.000 | 5 |
CaC2S2(OF)6 (mp-39536) | 0.5790 | 0.173 | 5 |
Zr2P3H4NO12 (mp-39770) | 0.5626 | 0.000 | 5 |
FeH4S2NO8 (mp-703668) | 0.4188 | 0.000 | 5 |
InP2H4NO8 (mp-698151) | 0.5968 | 0.238 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Eu Re_pv O |
Final Energy/Atom-8.8097 eV |
Corrected Energy-102.5251 eV
-102.5251 eV = -96.9068 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)