Final Magnetic Moment0.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.705 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.089 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBiO2 + SnO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4m2 [119] |
HallI 4 2 |
Point Group42m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 176.4 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 195.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 141.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 246.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 264.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 282.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 321.9 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 158.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 299.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 282.2 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 197.0 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 321.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 158.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 158.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 325.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 158.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 158.7 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 147.8 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 229.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 141.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 260.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 317.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 123.5 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 49.3 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 195.1 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 260.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 282.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 321.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 344.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 299.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 194.0 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 335.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 88.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 194.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 17.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 88.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 335.1 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 229.3 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 264.5 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 264.5 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 88.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 17.6 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 49.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 88.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 246.3 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 269.5 |
BN (mp-984) | <0 0 1> | <1 1 1> | 269.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 229.3 |
BN (mp-984) | <1 1 1> | <1 0 1> | 344.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 123.5 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
204 | 66 | 92 | 0 | 0 | 0 |
66 | 204 | 92 | 0 | 0 | 0 |
92 | 92 | 161 | 0 | 0 | 0 |
0 | 0 | 0 | 23 | 0 | 0 |
0 | 0 | 0 | 0 | 23 | 0 |
0 | 0 | 0 | 0 | 0 | 25 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
6.6 | -0.6 | -3.4 | 0 | 0 | 0 |
-0.6 | 6.6 | -3.4 | 0 | 0 | 0 |
-3.4 | -3.4 | 10.1 | 0 | 0 | 0 |
0 | 0 | 0 | 44.3 | 0 | 0 |
0 | 0 | 0 | 0 | 44.3 | 0 |
0 | 0 | 0 | 0 | 0 | 40.8 |
Shear Modulus GV35 GPa |
Bulk Modulus KV119 GPa |
Shear Modulus GR29 GPa |
Bulk Modulus KR118 GPa |
Shear Modulus GVRH32 GPa |
Bulk Modulus KVRH118 GPa |
Elastic Anisotropy1.02 |
Poisson's Ratio0.37 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TiVO4 (mp-780818) | 0.2680 | 0.042 | 3 |
TiSnO4 (mp-773864) | 0.0949 | 0.066 | 3 |
TiCrO4 (mp-773450) | 0.1943 | 0.071 | 3 |
NbFeO4 (mp-774156) | 0.1657 | 0.023 | 3 |
TiMnO4 (mp-775296) | 0.2280 | 0.053 | 3 |
LiFe5(OF2)4 (mp-782691) | 0.3266 | 0.081 | 4 |
AlMo(WO4)2 (mvc-685) | 0.4620 | 0.076 | 4 |
AlV(WO4)2 (mvc-704) | 0.4452 | 0.014 | 4 |
AlFe(WO4)2 (mvc-836) | 0.4518 | 0.069 | 4 |
MnAl(WO4)2 (mvc-648) | 0.4671 | 0.062 | 4 |
K2O (mp-684904) | 0.2895 | 0.040 | 2 |
ZrO2 (mp-754403) | 0.2606 | 0.015 | 2 |
FeO2 (mp-25517) | 0.3009 | 0.165 | 2 |
SnO2 (mp-755071) | 0.2887 | 0.057 | 2 |
TiO2 (mp-390) | 0.2895 | 0.006 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sn_d Bi O |
Final Energy/Atom-5.8518 eV |
Corrected Energy-37.9198 eV
-37.9198 eV = -35.1107 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)