material

CoSb2

ID:

mp-755

DOI:

10.17188/1289663


Tags: Cobalt antimonide (1/2) - nano-sized Cobalt antimonide (1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.177 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.002 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.19 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CoSb + CoSb3
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21/c [14]
Hall
-P 2ybc
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 42614 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Fe3O4 (mp-19306) <1 0 0> <1 1 -1> 0.016 290.8
SrTiO3 (mp-4651) <1 0 1> <1 0 1> 0.023 215.4
SiC (mp-11714) <0 0 1> <1 0 1> 0.033 215.4
SiC (mp-7631) <0 0 1> <1 0 1> 0.033 215.4
GaN (mp-804) <0 0 1> <1 0 1> 0.036 71.8
CdS (mp-672) <1 0 1> <0 1 0> 0.037 229.5
CdS (mp-672) <0 0 1> <1 0 1> 0.047 215.4
GaN (mp-804) <1 1 1> <1 1 1> 0.048 244.0
LiGaO2 (mp-5854) <1 1 0> <1 0 1> 0.065 143.6
CsI (mp-614603) <1 1 1> <1 0 1> 0.070 215.4
C (mp-48) <0 0 1> <1 0 -1> 0.070 175.3
PbS (mp-21276) <1 0 0> <1 1 -1> 0.075 290.8
Te2Mo (mp-602) <0 0 1> <1 0 1> 0.075 143.6
BN (mp-984) <1 0 1> <0 1 1> 0.076 340.5
YVO4 (mp-19133) <1 1 0> <1 0 -1> 0.082 131.5
TiO2 (mp-2657) <1 0 0> <1 0 -1> 0.084 262.9
LiGaO2 (mp-5854) <0 1 0> <1 0 -1> 0.084 131.5
ZrO2 (mp-2858) <1 1 -1> <0 1 1> 0.088 227.0
KCl (mp-23193) <1 1 0> <1 0 -1> 0.094 175.3
SiC (mp-11714) <1 0 0> <0 1 1> 0.101 283.7
NdGaO3 (mp-3196) <1 0 1> <1 0 1> 0.106 215.4
CdWO4 (mp-19387) <1 0 0> <0 1 1> 0.116 340.5
LiGaO2 (mp-5854) <0 1 1> <1 1 -1> 0.121 174.5
ZnO (mp-2133) <0 0 1> <0 0 1> 0.126 293.4
BaTiO3 (mp-5986) <1 0 0> <1 0 -1> 0.127 219.1
Cu (mp-30) <1 1 1> <1 0 0> 0.127 337.5
CdS (mp-672) <1 1 1> <0 0 1> 0.133 209.6
Bi2Se3 (mp-541837) <0 0 1> <1 0 1> 0.135 215.4
CdWO4 (mp-19387) <0 0 1> <0 1 1> 0.144 340.5
TeO2 (mp-2125) <0 0 1> <0 1 0> 0.156 191.2
TbScO3 (mp-31119) <1 1 0> <0 1 0> 0.163 191.2
C (mp-48) <1 0 0> <0 0 1> 0.164 209.6
Ga2O3 (mp-886) <1 0 0> <1 0 -1> 0.170 219.1
SrTiO3 (mp-4651) <1 0 0> <0 1 0> 0.180 267.7
DyScO3 (mp-31120) <1 1 0> <0 1 0> 0.196 191.2
Ni (mp-23) <1 0 0> <0 0 1> 0.205 209.6
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.211 209.6
BaTiO3 (mp-5986) <1 0 1> <0 1 0> 0.212 306.0
GdScO3 (mp-5690) <1 1 0> <0 1 0> 0.214 191.2
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.218 293.4
BaTiO3 (mp-5986) <0 0 1> <0 1 0> 0.218 191.2
GaSe (mp-1943) <0 0 1> <0 0 1> 0.229 125.7
BN (mp-984) <0 0 1> <1 0 0> 0.230 210.9
LaAlO3 (mp-2920) <0 0 1> <1 0 -1> 0.239 306.8
Mg (mp-153) <0 0 1> <0 0 1> 0.245 209.6
ZrO2 (mp-2858) <0 1 0> <0 1 0> 0.260 306.0
C (mp-66) <1 1 1> <1 0 0> 0.278 337.5
Mg (mp-153) <1 1 1> <1 1 1> 0.279 244.0
C (mp-66) <1 0 0> <0 0 1> 0.283 167.7
Ge (mp-32) <1 0 0> <0 0 1> 0.288 167.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
183 41 61 0 28 0
41 229 47 0 9 0
61 47 194 0 -13 0
0 0 0 83 0 24
28 9 -13 0 54 0
0 0 0 24 0 59
Compliance Tensor Sij (10-12Pa-1)
7.1 -0.6 -2.3 0 -4.2 0
-0.6 4.7 -1 0 -0.7 0
-2.3 -1 6.3 0 2.9 0
0 0 0 13.6 0 -5.6
-4.2 -0.7 2.9 0 21.6 0
0 0 0 -5.6 0 19.3
Shear Modulus GV
70 GPa
Bulk Modulus KV
101 GPa
Shear Modulus GR
60 GPa
Bulk Modulus KR
98 GPa
Shear Modulus GVRH
65 GPa
Bulk Modulus KVRH
99 GPa
Elastic Anisotropy
0.86
Poisson's Ratio
0.23

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CoGeTe (mp-3715) 0.4144 0.000 3
GeTeRh (mp-607818) 0.4906 0.000 3
FeAsS (mp-561511) 0.4799 0.000 3
PRuS (mp-1095584) 0.4793 0.005 3
TeAsRu (mp-1095634) 0.3788 0.000 3
Li8Mn(O2F)2 (mp-780086) 0.6420 0.071 4
Sr2Li2NiO4 (mp-769674) 0.5684 0.091 4
Na2Li3CoO4 (mp-540990) 0.7222 0.000 4
Li3CaMnN3 (mp-569112) 0.6525 0.000 4
LiCaGaN2 (mp-570948) 0.6931 0.000 4
Bi2Rh (mp-23217) 0.0938 0.000 2
CoAs2 (mp-2715) 0.2620 0.000 2
Sb2Rh (mp-2682) 0.2060 0.000 2
CoP2 (mp-14285) 0.3589 0.000 2
Sb2Ir (mp-1247) 0.3021 0.000 2
NaZr2SN2Cl (mp-679669) 0.6774 0.077 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Co Sb
Final Energy/Atom
-5.2986 eV
Corrected Energy
-63.5837 eV
-63.5837 eV = -63.5837 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 42614
  • 624906
  • 43500
  • 63553
  • 624891
  • 161492
Submitted by
User remarks:
  • Cobalt antimonide (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)