Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.784 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.042 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToYCl3 + BaCl2 |
Band Gap4.581 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <1 0 0> | 277.5 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 109.8 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 118.3 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 277.5 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 277.5 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 109.8 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 171.1 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 277.5 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 109.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 277.5 |
BN (mp-984) | <0 0 1> | <1 0 -1> | 109.8 |
BN (mp-984) | <1 1 1> | <1 0 0> | 277.5 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 219.5 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 92.5 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 150.2 |
TeO2 (mp-2125) | <1 0 0> | <1 0 -1> | 219.5 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 92.5 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 0> | 150.2 |
C (mp-66) | <1 1 0> | <1 0 -1> | 109.8 |
MgO (mp-1265) | <1 0 0> | <0 1 1> | 161.6 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 277.5 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 185.0 |
PbSe (mp-2201) | <1 1 1> | <1 0 0> | 277.5 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 277.5 |
Ni (mp-23) | <1 1 1> | <1 0 1> | 171.1 |
PbSe (mp-2201) | <1 1 0> | <1 0 -1> | 109.8 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 -1> | 219.5 |
Au (mp-81) | <1 1 0> | <1 0 -1> | 219.5 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 277.5 |
CdSe (mp-2691) | <1 1 0> | <1 0 -1> | 109.8 |
C (mp-48) | <0 0 1> | <0 1 0> | 236.6 |
ZrO2 (mp-2858) | <0 1 1> | <1 0 0> | 277.5 |
SiC (mp-8062) | <1 1 0> | <1 0 -1> | 109.8 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 277.5 |
TiO2 (mp-390) | <1 0 1> | <1 0 0> | 277.5 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 277.5 |
GaSb (mp-1156) | <1 1 0> | <1 0 -1> | 109.8 |
ZnO (mp-2133) | <1 1 0> | <0 1 0> | 118.3 |
Cu (mp-30) | <1 1 0> | <1 0 -1> | 109.8 |
Cu (mp-30) | <1 1 1> | <1 0 0> | 92.5 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 277.5 |
Fe2O3 (mp-24972) | <0 0 1> | <1 0 0> | 92.5 |
ZnTe (mp-2176) | <1 1 0> | <1 0 -1> | 109.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaFeF5 (mvc-14316) | 0.1947 | 0.000 | 3 |
CaCrF5 (mvc-14169) | 0.2076 | 0.000 | 3 |
BaYI5 (mp-754144) | 0.1712 | 0.076 | 3 |
BaYBr5 (mp-753663) | 0.1024 | 0.057 | 3 |
CaCrF5 (mp-622572) | 0.2104 | 0.000 | 3 |
U3O8 (mp-698) | 0.7499 | 0.003 | 2 |
U2O5 (mp-647814) | 0.6990 | 0.017 | 2 |
Np2O5 (mp-554714) | 0.6720 | 0.000 | 2 |
U3O8 (mp-560402) | 0.6632 | 0.005 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Y_sv Cl |
Final Energy/Atom-4.8776 eV |
Corrected Energy-68.2857 eV
-68.2857 eV = -68.2857 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)