Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.796 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.053 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCs2O + BaO |
Band Gap1.456 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Al (mp-134) | <1 1 0> | <0 0 1> | 207.5 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 311.3 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 253.9 |
TeO2 (mp-2125) | <0 1 1> | <1 0 1> | 297.8 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 1> | 288.9 |
TiO2 (mp-2657) | <0 0 1> | <0 1 1> | 192.6 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 207.5 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 259.4 |
C (mp-66) | <1 0 0> | <0 0 1> | 51.9 |
C (mp-66) | <1 1 0> | <1 1 0> | 234.5 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 253.9 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 253.9 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 1> | 297.8 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 311.3 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 311.3 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 155.6 |
KP(HO2)2 (mp-23959) | <0 1 1> | <0 0 1> | 103.8 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 259.4 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 51.9 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 311.3 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 311.3 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 253.9 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 253.9 |
TbScO3 (mp-31119) | <1 1 1> | <1 0 1> | 297.8 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 207.5 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 243.4 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 311.3 |
PbSe (mp-2201) | <1 0 0> | <0 1 1> | 192.6 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 207.5 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 259.4 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 0> | 243.4 |
BaTiO3 (mp-5986) | <1 1 1> | <1 1 0> | 117.2 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 253.9 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 253.9 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 311.3 |
Au (mp-81) | <1 0 0> | <0 1 0> | 243.4 |
Au (mp-81) | <1 1 0> | <0 1 0> | 243.4 |
CdSe (mp-2691) | <1 0 0> | <0 1 1> | 192.6 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 311.3 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 311.3 |
C (mp-48) | <0 0 1> | <0 1 0> | 243.4 |
C (mp-48) | <1 1 1> | <0 1 0> | 243.4 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 297.8 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 297.8 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 297.8 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 198.5 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 297.8 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 192.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 311.3 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 297.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K2CdO2 (mp-27742) | 0.3606 | 0.000 | 3 |
Na3(NiO2)2 (mp-850400) | 0.4777 | 0.097 | 3 |
Cs2CaO2 (mp-753803) | 0.4320 | 0.093 | 3 |
KSbO2 (mp-10417) | 0.5082 | 0.000 | 3 |
Rb2CdO2 (mp-28364) | 0.3591 | 0.000 | 3 |
Li4Mn(OF)2 (mp-767317) | 0.6688 | 0.092 | 4 |
Sr3MgGeN4 (mp-567398) | 0.6591 | 0.000 | 4 |
Na2Li2CoO4 (mp-763254) | 0.6679 | 0.073 | 4 |
CuBiPtS3 (mp-865018) | 0.6517 | 0.000 | 4 |
Na2Li2FeO4 (mp-25538) | 0.5929 | 0.060 | 4 |
Nb4O5 (mp-28212) | 0.7006 | 0.024 | 2 |
Re2P5 (mp-27736) | 0.6720 | 0.000 | 2 |
LiP5 (mp-32760) | 0.7099 | 0.099 | 2 |
LiP5 (mp-2412) | 0.7058 | 0.013 | 2 |
FeS2 (mp-850009) | 0.6761 | 0.438 | 2 |
Si (mp-676011) | 0.7207 | 0.447 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Ba_sv O |
Final Energy/Atom-4.2363 eV |
Corrected Energy-90.3449 eV
-90.3449 eV = -84.7266 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)