Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-1.342 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.097 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.74 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
LiCuO
Band Gap
0.953 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmcm [63]
Hall
-C 2c 2
Point Group
mmm
Crystal System
orthorhombic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-11714) <0 0 1> <1 1 0> -0.075 188.2
SiC (mp-7631) <0 0 1> <1 1 0> -0.072 188.2
MoS2 (mp-1434) <1 1 0> <1 1 0> -0.063 235.2
Mg (mp-153) <1 1 0> <1 1 0> -0.060 235.2
BN (mp-984) <1 1 1> <1 1 1> -0.031 170.6
TeO2 (mp-2125) <0 0 1> <1 1 1> -0.021 227.4
TbScO3 (mp-31119) <0 0 1> <1 1 1> -0.007 284.3
NdGaO3 (mp-3196) <0 1 1> <1 0 0> 0.001 263.7
Te2W (mp-22693) <0 1 0> <0 1 1> 0.002 108.2
DyScO3 (mp-31120) <0 0 1> <1 1 1> 0.005 284.3
Al2O3 (mp-1143) <1 0 1> <1 0 0> 0.005 131.8
BaTiO3 (mp-5986) <1 0 0> <0 1 1> 0.007 252.5
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.012 95.8
LiGaO2 (mp-5854) <1 0 1> <0 1 1> 0.012 180.4
TiO2 (mp-2657) <0 0 1> <0 1 1> 0.013 108.2
Fe2O3 (mp-24972) <1 0 0> <0 1 0> 0.016 285.8
LiAlO2 (mp-3427) <1 1 0> <0 1 0> 0.017 235.4
TePb (mp-19717) <1 0 0> <0 1 1> 0.018 216.4
Fe2O3 (mp-24972) <1 1 1> <0 1 0> 0.018 252.2
YAlO3 (mp-3792) <1 0 0> <0 1 0> 0.018 319.4
BaTiO3 (mp-5986) <1 1 0> <0 1 0> 0.018 168.1
GaP (mp-2490) <1 0 0> <0 1 1> 0.019 180.4
Si (mp-149) <1 0 0> <0 1 1> 0.020 180.4
CeO2 (mp-20194) <1 0 0> <0 1 1> 0.021 180.4
MoSe2 (mp-1634) <1 0 0> <0 0 1> 0.022 255.3
LiTaO3 (mp-3666) <1 0 1> <1 0 0> 0.024 307.6
CdWO4 (mp-19387) <1 0 0> <1 0 1> 0.024 217.2
Te2W (mp-22693) <0 1 1> <0 1 0> 0.024 117.7
TbScO3 (mp-31119) <1 1 1> <1 1 1> 0.025 284.3
LiAlO2 (mp-3427) <0 0 1> <0 1 1> 0.025 108.2
SiO2 (mp-6930) <1 0 0> <0 1 0> 0.026 218.5
LiNbO3 (mp-3731) <1 0 1> <1 0 0> 0.027 307.6
Ge (mp-32) <1 1 1> <0 1 1> 0.027 288.6
Ag (mp-124) <1 1 1> <0 1 1> 0.027 180.4
CaF2 (mp-2741) <1 0 0> <0 1 1> 0.028 180.4
TiO2 (mp-2657) <1 0 1> <1 1 1> 0.029 227.4
GaAs (mp-2534) <1 1 1> <0 1 1> 0.030 288.6
DyScO3 (mp-31120) <1 1 1> <1 1 1> 0.030 284.3
MgO (mp-1265) <1 1 1> <0 1 0> 0.031 218.5
TbScO3 (mp-31119) <0 1 1> <0 1 0> 0.032 218.5
LaF3 (mp-905) <1 0 0> <0 1 0> 0.033 319.4
Au (mp-81) <1 1 1> <0 1 1> 0.033 180.4
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.034 351.1
CdWO4 (mp-19387) <1 1 1> <0 0 1> 0.034 255.3
LiNbO3 (mp-3731) <1 1 0> <0 0 1> 0.034 127.7
ZnSe (mp-1190) <1 1 1> <0 1 1> 0.034 288.6
GdScO3 (mp-5690) <1 1 1> <1 1 1> 0.035 284.3
TbScO3 (mp-31119) <1 0 1> <0 1 0> 0.036 168.1
MgO (mp-1265) <1 0 0> <0 1 0> 0.036 269.0
KCl (mp-23193) <1 1 0> <1 0 0> 0.037 175.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
74 24 12 0 0 0
24 76 29 0 0 0
12 29 63 0 0 0
0 0 0 13 0 0
0 0 0 0 16 0
0 0 0 0 0 -25
Compliance Tensor Sij (10-12Pa-1)
15.1 -4.3 -0.9 0 0 0
-4.3 17.1 -6.9 0 0 0
-0.9 -6.9 19.1 0 0 0
0 0 0 76.9 0 0
0 0 0 0 61.9 0
0 0 0 0 0 -39.9
Shear Modulus GV
11 GPa
Bulk Modulus KV
38 GPa
Shear Modulus GR
27 GPa
Bulk Modulus KR
37 GPa
Shear Modulus GVRH
19 GPa
Bulk Modulus KVRH
38 GPa
Elastic Anisotropy
-3.00
Poisson's Ratio
0.28

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
72
U Values
--
Pseudopotentials
VASP PAW: Li_sv Cu_pv O
Final Energy/Atom
-4.7560 eV
Corrected Energy
-29.9406 eV
-29.9406 eV = -28.5361 eV (uncorrected energy) - 1.4046 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
User remarks:
  • supplementary compounds from MIT matgen database

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)