material

TiVO3

ID:

mp-755657


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
AFM
Formation Energy / Atom
-3.000 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.45 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3 [148]
Hall
-R 3
Point Group
3
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.001 208.6
GaN (mp-804) <0 0 1> <0 0 1> 0.002 278.2
LiGaO2 (mp-5854) <1 1 1> <0 0 1> 0.004 278.2
Ni (mp-23) <1 1 1> <0 0 1> 0.011 278.2
GaN (mp-804) <1 0 1> <0 0 1> 0.023 324.5
AlN (mp-661) <0 0 1> <0 0 1> 0.042 162.3
SiC (mp-8062) <1 1 1> <0 0 1> 0.047 301.4
TePb (mp-19717) <1 1 1> <0 0 1> 0.058 301.4
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.063 278.2
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.073 301.4
CdTe (mp-406) <1 1 1> <0 0 1> 0.080 301.4
TiO2 (mp-390) <1 0 1> <0 0 1> 0.082 278.2
LiNbO3 (mp-3731) <1 0 1> <1 0 1> 0.092 77.5
LiNbO3 (mp-3731) <1 1 1> <1 1 1> 0.095 130.1
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.100 370.9
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.101 92.7
InSb (mp-20012) <1 1 1> <0 0 1> 0.101 301.4
LiNbO3 (mp-3731) <1 1 0> <1 1 0> 0.105 128.0
LiNbO3 (mp-3731) <1 0 0> <1 0 0> 0.105 73.9
Mg (mp-153) <1 0 1> <0 0 1> 0.108 324.5
Te2W (mp-22693) <1 1 0> <1 0 0> 0.115 221.7
Au (mp-81) <1 1 0> <0 0 1> 0.119 370.9
TiO2 (mp-390) <1 0 0> <1 1 1> 0.123 260.2
LiAlO2 (mp-3427) <1 0 0> <0 0 1> 0.126 231.8
BaTiO3 (mp-5986) <1 0 1> <1 1 0> 0.127 256.0
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.130 139.1
Ag (mp-124) <1 0 0> <1 0 0> 0.132 295.7
Au (mp-81) <1 0 0> <1 0 0> 0.136 295.7
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.136 23.2
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.145 208.6
Cu (mp-30) <1 1 0> <1 0 0> 0.145 73.9
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.145 69.5
Ni (mp-23) <1 1 0> <1 0 0> 0.145 295.7
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.148 23.2
C (mp-48) <0 0 1> <0 0 1> 0.160 69.5
BaF2 (mp-1029) <1 1 0> <1 0 0> 0.162 221.7
GaN (mp-804) <1 0 0> <0 0 1> 0.165 185.5
Te2Mo (mp-602) <1 0 0> <1 0 0> 0.166 221.7
AlN (mp-661) <1 1 1> <1 1 1> 0.168 260.2
Ag (mp-124) <1 1 0> <0 0 1> 0.174 370.9
CaF2 (mp-2741) <1 1 0> <0 0 1> 0.175 347.7
LiGaO2 (mp-5854) <0 1 0> <0 0 1> 0.176 231.8
MgO (mp-1265) <1 1 1> <0 0 1> 0.177 92.7
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.184 92.7
SiC (mp-11714) <1 0 0> <0 0 1> 0.186 347.7
LiAlO2 (mp-3427) <1 0 1> <1 0 0> 0.190 295.7
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.214 69.5
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.226 347.7
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.228 115.9
CdS (mp-672) <1 0 1> <1 0 1> 0.233 232.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TiNiO3 (mp-18732) 0.1181 0.000 3
TiCoO3 (mp-558233) 0.2121 0.003 3
MgTiO3 (mp-3771) 0.2183 0.000 3
TiFeO3 (mp-818838) 0.2187 0.012 3
TiNiO3 (mp-556251) 0.1142 0.000 3
Mg2VWO6 (mvc-5881) 0.2815 0.022 4
Mg2MoWO6 (mvc-5910) 0.2932 0.036 4
Mg2TiWO6 (mvc-5939) 0.2687 0.125 4
Mg2CrWO6 (mvc-5960) 0.2887 0.670 4
InNi2SbO6 (mp-1078367) 0.2422 0.000 4
V2O3 (mp-715514) 0.3444 0.019 2
V2O3 (mp-714863) 0.3605 0.009 2
V2O3 (mp-562005) 0.3619 0.009 2
Fe2O3 (mp-24972) 0.3635 0.000 2
Fe2O3 (mp-796253) 0.3632 0.000 2
Li4Fe2TeWO12 (mp-768021) 0.4594 0.085 5
Li4Cr2TeWO12 (mp-775566) 0.5743 0.080 5
Li4MnV2WO12 (mp-773239) 0.6548 0.090 5
Li4Mn2TeWO12 (mp-768044) 0.5460 0.058 5
Li4V2CrTeO12 (mp-775632) 0.6021 0.104 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
V: 3.25 eV
Pseudopotentials
VASP PAW: Ti_pv V_pv O
Final Energy/Atom
-8.6127 eV
Corrected Energy
-93.6486 eV
Uncorrected energy = -86.1266 eV Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV Composition-based energy adjustment (-1.700 eV/atom x 2.0 atoms) = -3.4000 eV Corrected energy = -93.6486 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)