material

Nb5SiSn2

ID:

mp-7557

DOI:

10.17188/1290162


Tags: Niobium tin silicide (5/2/1)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.330 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.001 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.24 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
NbSn2 + Nb3Sn + Nb5Si3
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mcm [140]
Hall
-I 4 2c
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 16499 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ge3(BiO3)4 (mp-23560) <1 0 0> <0 0 1> 0.006 114.0
KP(HO2)2 (mp-23959) <0 0 1> <0 0 1> 0.008 227.9
SiC (mp-11714) <0 0 1> <1 0 0> 0.025 165.5
SiC (mp-7631) <0 0 1> <1 0 0> 0.028 165.5
KP(HO2)2 (mp-23959) <1 0 0> <0 0 1> 0.052 114.0
KP(HO2)2 (mp-23959) <0 1 0> <0 0 1> 0.057 227.9
Au (mp-81) <1 0 0> <0 0 1> 0.064 227.9
C (mp-66) <1 0 0> <0 0 1> 0.095 114.0
LiTaO3 (mp-3666) <0 0 1> <1 1 0> 0.103 234.0
Ag (mp-124) <1 0 0> <0 0 1> 0.181 227.9
LiNbO3 (mp-3731) <0 0 1> <1 1 0> 0.190 234.0
LiNbO3 (mp-3731) <1 0 0> <1 0 0> 0.205 220.6
Cu (mp-30) <1 1 1> <1 0 0> 0.251 275.8
BaTiO3 (mp-5986) <1 0 0> <1 0 1> 0.318 253.2
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.322 331.0
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.323 165.5
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.336 78.0
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.342 165.5
Ag (mp-124) <1 1 1> <1 0 0> 0.351 331.0
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.383 55.2
Mg (mp-153) <1 0 0> <1 0 0> 0.397 165.5
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.399 114.0
Ag (mp-124) <1 1 0> <1 0 0> 0.401 220.6
GaTe (mp-542812) <1 0 0> <1 0 0> 0.416 220.6
Au (mp-81) <1 1 0> <1 0 0> 0.420 220.6
YVO4 (mp-19133) <0 0 1> <1 1 0> 0.434 156.0
GaN (mp-804) <1 0 0> <1 0 0> 0.441 165.5
WS2 (mp-224) <1 0 1> <1 1 0> 0.444 234.0
Cu (mp-30) <1 1 0> <1 0 0> 0.445 55.2
SiO2 (mp-6930) <1 1 0> <1 0 0> 0.449 331.0
Cu (mp-30) <1 0 0> <1 1 0> 0.450 78.0
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.457 156.0
MgO (mp-1265) <1 0 0> <1 1 0> 0.458 234.0
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.490 55.2
TiO2 (mp-390) <0 0 1> <1 1 0> 0.493 234.0
AlN (mp-661) <1 1 1> <0 0 1> 0.494 114.0
GaN (mp-804) <1 1 0> <1 1 0> 0.525 234.0
BaTiO3 (mp-5986) <1 1 0> <1 1 0> 0.535 312.0
BN (mp-984) <1 1 1> <1 1 0> 0.540 312.0
ZrO2 (mp-2858) <1 1 0> <1 0 0> 0.542 275.8
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.555 220.6
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.603 110.3
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.618 220.6
CdS (mp-672) <1 0 0> <1 1 0> 0.627 312.0
SiC (mp-7631) <1 1 0> <1 0 0> 0.634 165.5
Ni (mp-23) <1 0 0> <1 0 0> 0.635 110.3
Ni (mp-23) <1 1 0> <1 1 0> 0.639 156.0
LiTaO3 (mp-3666) <1 0 0> <1 0 0> 0.639 220.6
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.654 55.2
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.666 227.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
297 93 93 0 0 0
93 289 106 0 0 0
93 106 289 0 0 0
0 0 0 95 0 0
0 0 0 0 67 0
0 0 0 0 0 67
Compliance Tensor Sij (10-12Pa-1)
4 -0.9 -0.9 0 0 0
-0.9 4.2 -1.2 0 0 0
-0.9 -1.2 4.2 0 0 0
0 0 0 10.6 0 0
0 0 0 0 15 0
0 0 0 0 0 15
Shear Modulus GV
84 GPa
Bulk Modulus KV
162 GPa
Shear Modulus GR
82 GPa
Bulk Modulus KR
162 GPa
Shear Modulus GVRH
83 GPa
Bulk Modulus KVRH
162 GPa
Elastic Anisotropy
0.17
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ti5FeSb2 (mp-30326) 0.3366 0.022 3
Ti5Sb2Rh (mp-16687) 0.3725 0.030 3
Ti5CuSb2 (mp-13020) 0.3679 0.002 3
Nb5GaSn2 (mp-17230) 0.2335 0.000 3
Ta5Ga3 (mp-568376) 0.4843 0.006 2
Ti3Sb (mp-569837) 0.4925 0.055 2
Nb5Ga3 (mp-570293) 0.4743 0.008 2
Nb5Ge3 (mp-16842) 0.5058 0.000 2
Nb5Si3 (mp-567996) 0.4993 0.045 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Nb_pv Si Sn_d
Final Energy/Atom
-8.3236 eV
Corrected Energy
-133.1776 eV
-133.1776 eV = -133.1776 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 16499
Submitted by
User remarks:
  • Niobium tin silicide (5/2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)