material

Ti3O4

ID:

mp-755875

DOI:

10.17188/1290249


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.133 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.058 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.71 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
TiO + Ti2O3
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmmm [65]
Hall
-C 2 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
C (mp-66) <1 0 0> <1 1 0> 0.011 152.7
LaAlO3 (mp-2920) <1 0 1> <0 1 0> 0.014 303.8
LaAlO3 (mp-2920) <0 0 1> <0 1 0> 0.023 303.8
CdSe (mp-2691) <1 1 1> <0 1 0> 0.042 268.0
GaSb (mp-1156) <1 1 1> <0 1 0> 0.043 268.0
ZnO (mp-2133) <1 0 1> <1 0 0> 0.046 99.1
ZrO2 (mp-2858) <1 0 1> <1 0 0> 0.046 173.4
NdGaO3 (mp-3196) <1 1 1> <0 1 1> 0.047 206.2
PbSe (mp-2201) <1 1 1> <0 1 0> 0.053 268.0
C (mp-48) <1 1 0> <0 1 0> 0.059 232.3
CdSe (mp-2691) <1 0 0> <0 1 1> 0.077 154.6
CsI (mp-614603) <1 0 0> <0 1 1> 0.077 309.2
GaSb (mp-1156) <1 0 0> <0 1 1> 0.082 154.6
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.086 272.5
SiC (mp-8062) <1 0 0> <0 1 1> 0.094 154.6
PbSe (mp-2201) <1 0 0> <0 1 1> 0.096 154.6
YVO4 (mp-19133) <1 1 0> <0 1 0> 0.101 196.6
SrTiO3 (mp-4651) <1 1 0> <0 1 1> 0.103 309.2
TePb (mp-19717) <1 0 0> <1 0 1> 0.106 217.3
NdGaO3 (mp-3196) <1 1 0> <0 1 1> 0.106 309.2
GaN (mp-804) <1 1 0> <0 1 0> 0.106 321.6
ZnTe (mp-2176) <1 0 0> <0 1 1> 0.118 154.6
GaSe (mp-1943) <1 0 0> <0 1 0> 0.122 268.0
InAs (mp-20305) <1 0 0> <0 1 1> 0.130 154.6
GaP (mp-2490) <1 0 0> <1 0 0> 0.131 272.5
TiO2 (mp-2657) <0 0 1> <0 1 1> 0.141 257.7
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.145 272.5
TiO2 (mp-2657) <1 0 1> <0 1 0> 0.151 303.8
LaAlO3 (mp-2920) <1 0 0> <1 0 1> 0.162 217.3
BaTiO3 (mp-5986) <0 0 1> <0 1 0> 0.162 143.0
PbS (mp-21276) <1 0 0> <0 1 0> 0.163 35.7
LiAlO2 (mp-3427) <0 0 1> <0 1 0> 0.171 357.4
InAs (mp-20305) <1 1 0> <1 0 0> 0.171 322.1
WSe2 (mp-1821) <1 0 0> <1 1 0> 0.171 152.7
LiAlO2 (mp-3427) <1 0 1> <1 0 0> 0.172 173.4
SrTiO3 (mp-4651) <1 1 1> <0 1 1> 0.176 206.2
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.178 198.2
Ga2O3 (mp-886) <1 1 1> <1 1 1> 0.180 171.6
ZnTe (mp-2176) <1 1 0> <1 0 0> 0.183 322.1
ZnO (mp-2133) <1 0 0> <0 0 1> 0.184 193.4
BN (mp-984) <1 1 1> <0 0 1> 0.192 241.7
InP (mp-20351) <1 0 0> <0 1 0> 0.198 35.7
SiC (mp-11714) <1 1 0> <1 1 0> 0.202 213.8
CdTe (mp-406) <1 0 0> <1 0 1> 0.203 217.3
YVO4 (mp-19133) <1 1 1> <1 0 0> 0.205 247.7
CdWO4 (mp-19387) <0 1 0> <1 1 0> 0.207 183.3
AlN (mp-661) <1 0 1> <1 0 0> 0.222 198.2
LiAlO2 (mp-3427) <1 0 0> <1 0 1> 0.222 163.0
InSb (mp-20012) <1 0 0> <1 0 1> 0.228 217.3
SiO2 (mp-6930) <0 0 1> <0 1 0> 0.236 196.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
253 72 164 0 0 0
72 425 58 0 0 0
164 58 352 0 0 0
0 0 0 51 0 0
0 0 0 0 128 0
0 0 0 0 0 69
Compliance Tensor Sij (10-12Pa-1)
5.8 -0.6 -2.6 0 0 0
-0.6 2.5 -0.1 0 0 0
-2.6 -0.1 4.1 0 0 0
0 0 0 19.6 0 0
0 0 0 0 7.8 0
0 0 0 0 0 14.5
Shear Modulus GV
99 GPa
Bulk Modulus KV
180 GPa
Shear Modulus GR
79 GPa
Bulk Modulus KR
177 GPa
Shear Modulus GVRH
89 GPa
Bulk Modulus KVRH
178 GPa
Elastic Anisotropy
1.22
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ti2ZnS4 (mvc-16628) 0.2160 0.174 3
MgTi2O4 (mvc-16746) 0.2096 0.102 3
Ti2ZnO4 (mvc-16752) 0.2366 0.303 3
Al(NiS2)2 (mvc-16791) 0.2319 0.190 3
Mg(FeO2)2 (mvc-16835) 0.2396 0.143 3
LiTiFeO4 (mp-762701) 0.3856 0.098 4
Li2TiV3O8 (mp-769560) 0.3971 0.068 4
Li2Cr3FeO8 (mp-779991) 0.4043 0.643 4
Li2MnCr3O8 (mp-781699) 0.3983 0.063 4
LiTi4VO8 (mp-768022) 0.2635 0.227 4
Fe3O4 (mp-612405) 0.4009 0.175 2
Zr3S4 (mp-684749) 0.4607 0.000 2
Ni3Cl4 (mp-1096772) 0.1467 0.265 2
Ni3Cl4 (mp-1096769) 0.2020 0.267 2
Ni3Cl4 (mp-1096770) 0.1497 0.265 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv O
Final Energy/Atom
-8.9513 eV
Corrected Energy
-65.4071 eV
Uncorrected energy = -62.6591 eV Composition-based energy adjustment (-0.687 eV/atom x 4.0 atoms) = -2.7480 eV Corrected energy = -65.4071 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)