Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.172 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.076 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBr2O3 + Ag3O4 + O2 |
Band Gap0.928 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 219.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 306.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 219.2 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 250.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 187.7 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 199.8 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 66.6 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 333.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 229.2 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 250.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 219.2 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 133.2 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 229.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 187.7 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 305.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 187.7 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 152.8 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 229.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 306.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 160.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 200.6 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 152.8 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 312.8 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 66.6 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 250.2 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 240.6 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 300.9 |
Te2W (mp-22693) | <1 1 0> | <1 0 1> | 229.2 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 219.2 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 240.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 306.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 175.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 250.2 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 62.6 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 250.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 219.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 219.2 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 187.7 |
Al (mp-134) | <1 1 0> | <0 1 0> | 200.6 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 187.7 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 306.8 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 187.7 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 187.7 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 50.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 350.7 |
BN (mp-984) | <0 0 1> | <1 1 0> | 240.6 |
BN (mp-984) | <1 0 1> | <1 1 1> | 182.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 219.2 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 150.5 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 219.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SmBeF4 (mp-505432) | 0.4201 | 0.359 | 3 |
ReHgO4 (mp-616597) | 0.3489 | 0.000 | 3 |
CaSO4 (mp-562260) | 0.3852 | 0.056 | 3 |
TlGaCl4 (mp-570609) | 0.3647 | 0.000 | 3 |
AlTlCl4 (mp-567716) | 0.4232 | 0.000 | 3 |
Sn3PO4F3 (mp-546757) | 0.5129 | 0.000 | 4 |
GaHg2SbCl4 (mp-568031) | 0.5941 | 0.001 | 4 |
SnS2(O3F)2 (mp-554599) | 0.6495 | 0.005 | 4 |
AlHg2SbCl4 (mp-570828) | 0.6038 | 0.000 | 4 |
RePbClO4 (mp-560625) | 0.6577 | 0.011 | 4 |
GaBr2 (mp-650841) | 0.7434 | 0.011 | 2 |
VCl4 (mp-570763) | 0.7317 | 0.004 | 2 |
Ca2Al2Si(HO4)2 (mp-686748) | 0.7249 | 0.000 | 5 |
PH4N(OF)2 (mp-706976) | 0.7400 | 0.000 | 5 |
RbSbS(O2F)2 (mp-554732) | 0.7415 | 0.000 | 5 |
BH11C4NClF4 (mp-559235) | 0.7420 | 0.113 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ag Br O |
Final Energy/Atom-3.7471 eV |
Corrected Energy-101.1681 eV
-101.1681 eV = -89.9315 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)