material

Cu(SbO2)2

ID:

mp-756132

DOI:

10.17188/1290358


Material Details

Final Magnetic Moment
4.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-1.488 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.103 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.26 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
SbO2 + Cu
Band Gap
0.298 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P42/mbc [135]
Hall
-P 4c 2ab
Point Group
4/mmm
Crystal System
tetragonal

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.003 79.5
Ni (mp-23) <1 0 0> <0 0 1> 0.004 158.9
C (mp-66) <1 0 0> <1 0 1> 0.004 190.5
Y3Fe5O12 (mp-19648) <1 0 0> <0 0 1> 0.005 158.9
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.005 79.5
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.007 222.8
Au (mp-81) <1 1 0> <1 1 0> 0.007 74.3
SrTiO3 (mp-4651) <1 1 1> <1 0 0> 0.008 210.1
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.011 315.1
SiC (mp-11714) <0 0 1> <1 0 0> 0.012 262.6
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.012 262.6
BaTiO3 (mp-5986) <1 1 1> <1 0 0> 0.012 315.1
SiC (mp-7631) <0 0 1> <1 0 0> 0.014 262.6
Ag (mp-124) <1 1 0> <1 1 0> 0.016 74.3
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.017 222.8
LaAlO3 (mp-2920) <1 0 0> <1 0 1> 0.017 285.8
Au (mp-81) <1 0 0> <0 0 1> 0.018 158.9
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.018 315.1
ZrO2 (mp-2858) <1 0 0> <1 0 1> 0.019 285.8
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.019 238.4
SiC (mp-11714) <1 0 0> <1 1 1> 0.022 217.6
CdS (mp-672) <1 0 0> <1 0 1> 0.023 285.8
CdTe (mp-406) <1 0 0> <1 0 0> 0.024 262.6
TePb (mp-19717) <1 0 0> <1 0 0> 0.025 262.6
BN (mp-984) <1 0 0> <1 0 0> 0.026 210.1
ZnO (mp-2133) <1 0 0> <1 1 0> 0.026 297.1
GaTe (mp-542812) <1 0 1> <1 1 0> 0.028 297.1
InSb (mp-20012) <1 0 0> <1 0 0> 0.029 262.6
GaN (mp-804) <1 0 1> <1 0 0> 0.030 210.1
NaCl (mp-22862) <1 0 0> <0 0 1> 0.030 158.9
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.030 262.6
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.032 315.1
PbSe (mp-2201) <1 1 0> <1 1 0> 0.034 222.8
ZrO2 (mp-2858) <1 0 -1> <1 0 1> 0.037 285.8
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.037 262.6
Mg (mp-153) <1 0 1> <1 0 0> 0.038 210.1
AlN (mp-661) <1 0 0> <1 1 0> 0.040 222.8
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.040 238.4
SiO2 (mp-6930) <1 1 0> <0 0 1> 0.044 238.4
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.046 157.6
LiNbO3 (mp-3731) <0 0 1> <1 0 1> 0.047 95.3
KCl (mp-23193) <1 1 1> <1 0 1> 0.048 285.8
GaSb (mp-1156) <1 1 0> <1 1 0> 0.048 222.8
PbSe (mp-2201) <1 0 0> <0 0 1> 0.048 79.5
C (mp-48) <1 1 0> <1 1 0> 0.049 297.1
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.051 158.9
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.051 315.1
YAlO3 (mp-3792) <0 0 1> <1 0 1> 0.051 285.8
DyScO3 (mp-31120) <1 1 1> <1 0 0> 0.051 210.1
BaTiO3 (mp-5986) <1 1 0> <1 1 1> 0.053 217.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
120 15 15 0 0 0
15 18 13 0 0 0
15 13 18 0 0 0
0 0 0 10 0 0
0 0 0 0 2 0
0 0 0 0 0 2
Compliance Tensor Sij (10-12Pa-1)
9.4 -4.5 -4.5 0 0 0
-4.5 113.8 -78 0 0 0
-4.5 -78 113.8 0 0 0
0 0 0 98.5 0 0
0 0 0 0 510.2 0
0 0 0 0 0 510.2
Shear Modulus GV
10 GPa
Bulk Modulus KV
27 GPa
Shear Modulus GR
3 GPa
Bulk Modulus KR
16 GPa
Shear Modulus GVRH
7 GPa
Bulk Modulus KVRH
21 GPa
Elastic Anisotropy
11.84
Poisson's Ratio
0.36

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
32
U Values
--
Pseudopotentials
VASP PAW: Cu_pv Sb O
Final Energy/Atom
-5.6708 eV
Corrected Energy
-170.0200 eV
-170.0200 eV = -158.7834 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
User remarks:
  • supplementary compounds from MIT matgen database

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)