Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.996 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.595 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 1> | <1 0 0> | 115.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 85.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 256.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 85.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 115.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 85.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 256.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 256.4 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 256.4 |
C (mp-66) | <1 0 0> | <0 0 1> | 256.4 |
Al (mp-134) | <1 1 1> | <0 0 1> | 85.5 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 115.8 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 256.4 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 256.4 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 85.5 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 256.4 |
C (mp-66) | <1 1 0> | <1 0 1> | 143.9 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 115.8 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 256.4 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 85.5 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 256.4 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 115.8 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 85.5 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 256.4 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 170.9 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 256.4 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 256.4 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 256.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.77 | 0.00 | 0.00 |
-0.00 | 3.77 | -0.00 |
0.00 | -0.00 | 3.62 |
Dielectric Tensor εij (total) |
||
---|---|---|
12.90 | -0.00 | 0.00 |
-0.00 | 12.90 | -0.00 |
0.00 | -0.00 | 11.42 |
Polycrystalline dielectric constant
εpoly∞
3.72
|
Polycrystalline dielectric constant
εpoly
12.41
|
Refractive Index n1.93 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca3WO6 (mp-781505) | 0.2240 | 0.000 | 3 |
Mn3WO6 (mp-19158) | 0.4725 | 0.000 | 3 |
Ca3UO6 (mp-14252) | 0.4545 | 0.000 | 3 |
Na3CrCl6 (mp-28360) | 0.3338 | 0.000 | 3 |
K3SmN6 (mp-1080840) | 0.3640 | 1.924 | 3 |
Ca2TeWO6 (mvc-5060) | 0.4592 | 0.263 | 4 |
Ca2MnWO6 (mvc-16535) | 0.4526 | 0.021 | 4 |
Ca2NiWO6 (mvc-16546) | 0.3780 | 0.102 | 4 |
Ca3Zn3(TeO6)2 (mp-555961) | 0.3787 | 0.120 | 4 |
Ca2MnWO6 (mvc-12168) | 0.5035 | 0.022 | 4 |
RhN2 (mp-20304) | 0.5873 | 0.107 | 2 |
ReN2 (mp-1019078) | 0.5470 | 0.144 | 2 |
LiO2 (mp-1018789) | 0.5618 | 0.088 | 2 |
IrN2 (mp-13076) | 0.5819 | 0.200 | 2 |
CrN2 (mp-1080200) | 0.5444 | 0.151 | 2 |
CaLaTaCrO6 (mvc-10008) | 0.6251 | 0.035 | 5 |
CaLaFeSbO6 (mvc-8959) | 0.6465 | 0.001 | 5 |
CaLaFeBiO6 (mvc-8967) | 0.5742 | 0.057 | 5 |
CaLaFeWO6 (mvc-9032) | 0.6272 | 0.023 | 5 |
CaLaCrBiO6 (mvc-9978) | 0.5845 | 0.198 | 5 |
Run TypeGGA+U |
Energy Cutoff700 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Sr_sv W_pv O |
Final Energy/Atom-6.9106 eV |
Corrected Energy-155.3405 eV
-155.3405 eV = -138.2110 eV (uncorrected energy) - 8.7020 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)