Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.024 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.053 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLaBr3 + SrBr2 |
Band Gap2.736 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 308.1 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 218.0 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 265.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 351.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 175.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 246.0 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 175.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 105.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 316.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 140.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 276.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 276.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 351.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 351.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 281.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 246.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 246.5 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 145.3 |
SiO2 (mp-6930) | <1 1 1> | <1 1 -1> | 261.6 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 276.6 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 276.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 281.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 175.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 140.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 246.0 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 276.6 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 276.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 316.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 140.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 316.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 316.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 246.0 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 116.5 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 290.7 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 308.1 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 308.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 351.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 316.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 218.0 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 276.6 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 290.7 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 276.6 |
Te2Mo (mp-602) | <1 0 1> | <1 0 -1> | 276.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 351.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 69.1 |
Bi2Te3 (mp-34202) | <1 0 0> | <1 0 -1> | 138.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 175.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 316.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 140.5 |
BN (mp-984) | <1 1 0> | <1 0 -1> | 69.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaLaBr5 (mp-770405) | 0.1911 | 0.073 | 3 |
Ba2LaI7 (mp-772158) | 0.5033 | 0.054 | 3 |
SrLaI5 (mp-755393) | 0.2172 | 0.047 | 3 |
SrLaCl5 (mp-768963) | 0.2294 | 0.075 | 3 |
RbNd2I5 (mp-570360) | 0.6556 | 0.132 | 3 |
Mg2Si3 (mp-1073256) | 0.6754 | 0.149 | 2 |
Tm7Cl15 (mp-680292) | 0.7030 | 0.267 | 2 |
Mg2Si3 (mp-1073121) | 0.6165 | 0.218 | 2 |
Mg2Si3 (mp-1072996) | 0.6604 | 0.220 | 2 |
Mg2Si3 (mp-1073041) | 0.6752 | 0.196 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv La Br |
Final Energy/Atom-4.1393 eV |
Corrected Energy-57.9499 eV
-57.9499 eV = -57.9499 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)