Final Magnetic Moment1.705 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.033 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.056 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.98 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu2P2O7 + Te2P2O9 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 322.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 193.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 225.7 |
AlN (mp-661) | <1 0 1> | <1 1 -1> | 254.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 161.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 290.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 207.8 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 150.3 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 258.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 257.9 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 75.1 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 244.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 277.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 225.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 225.7 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 341.6 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 150.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 161.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 354.6 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 207.8 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 290.2 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 161.2 |
Te2W (mp-22693) | <1 0 1> | <1 0 -1> | 207.8 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 96.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 354.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 207.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 233.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 225.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 292.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 129.0 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 300.6 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 323.3 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 277.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 354.6 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 75.1 |
BN (mp-984) | <1 0 0> | <0 0 1> | 225.7 |
BN (mp-984) | <1 1 0> | <1 0 1> | 300.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 193.4 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 292.8 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 257.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 257.9 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 225.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 341.6 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 300.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 323.3 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 290.2 |
Al (mp-134) | <1 0 0> | <1 0 -1> | 277.0 |
Al (mp-134) | <1 1 1> | <0 0 1> | 193.4 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 -1> | 69.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 322.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AgAsO3 (mp-775767) | 0.5730 | 0.037 | 3 |
MnAsO4 (mp-543097) | 0.5458 | 0.031 | 3 |
MnPO4 (mp-540007) | 0.5845 | 0.003 | 3 |
Cd(PO3)2 (mp-4659) | 0.5808 | 0.000 | 3 |
MnPO4 (mp-566973) | 0.5849 | 0.003 | 3 |
CuSb(PO4)2 (mp-755148) | 0.3890 | 0.074 | 4 |
MnCu3(PO4)4 (mp-775168) | 0.3851 | 0.162 | 4 |
CuSn(PO4)2 (mp-758849) | 0.4385 | 0.039 | 4 |
Mn3Cu(PO4)4 (mp-772001) | 0.3719 | 0.017 | 4 |
MnSb3(PO4)4 (mp-774091) | 0.3448 | 0.213 | 4 |
MnFeCo(PO4)3 (mp-764410) | 0.5323 | 0.027 | 5 |
MnFeCo(PO4)3 (mp-764392) | 0.5654 | 0.028 | 5 |
MnFeCo(PO4)3 (mp-763496) | 0.5698 | 0.026 | 5 |
MnFeCo(PO4)3 (mp-764415) | 0.5421 | 0.035 | 5 |
MnFeCo(PO4)3 (mp-763446) | 0.5701 | 0.033 | 5 |
K3Na3TeP6(HO4)6 (mp-720804) | 0.7393 | 0.030 | 6 |
Na3CaSc3Zn(SiO3)8 (mp-720987) | 0.6762 | 0.230 | 6 |
NaCoBP2H2O9 (mp-601388) | 0.7079 | 0.052 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cu_pv Te P O |
Final Energy/Atom-6.3695 eV |
Corrected Energy-164.1046 eV
-164.1046 eV = -152.8680 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)