Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.791 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.080 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTmAsO4 |
Band Gap3.575 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 223.6 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 276.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 276.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 223.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 140.9 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 214.6 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 186.5 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 140.9 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 223.6 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 257.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 167.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 343.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 322.4 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 230.3 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 140.9 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 184.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 186.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 276.3 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 230.3 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 223.6 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 314.8 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 140.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 230.3 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 273.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 230.3 |
BN (mp-984) | <1 0 0> | <0 1 1> | 251.8 |
BN (mp-984) | <1 0 1> | <0 1 0> | 214.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 140.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 257.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 300.5 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 223.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 167.7 |
GaN (mp-804) | <1 0 1> | <1 1 -1> | 253.5 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 300.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 326.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 322.4 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 211.4 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 223.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 281.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 279.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 276.3 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 273.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 276.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 128.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 279.5 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 300.5 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 139.9 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 279.5 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 223.6 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 322.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HoAsO4 (mp-777787) | 0.1109 | 0.069 | 3 |
BiAsO4 (mp-27911) | 0.2693 | 0.000 | 3 |
CdSeO4 (mp-756703) | 0.2636 | 0.061 | 3 |
SmAsO4 (mp-754876) | 0.2738 | 0.037 | 3 |
GdAsO4 (mp-754079) | 0.1810 | 0.046 | 3 |
Sm2SiTeO4 (mp-17812) | 0.4839 | 0.007 | 4 |
NaSm(PS3)2 (mp-561232) | 0.4465 | 0.000 | 4 |
LaTlGeSe4 (mp-684022) | 0.4770 | 0.002 | 4 |
BaLaGaO4 (mp-541280) | 0.4535 | 0.007 | 4 |
KY(PSe3)2 (mp-571057) | 0.4745 | 0.000 | 4 |
Nd2O5 (mp-985608) | 0.5504 | 0.028 | 2 |
TlBr2 (mp-27398) | 0.6022 | 0.000 | 2 |
InI2 (mp-29312) | 0.5767 | 0.000 | 2 |
InBr2 (mp-568108) | 0.6423 | 0.000 | 2 |
GaCl2 (mp-568848) | 0.6692 | 0.000 | 2 |
SrLaTl(AsO4)2 (mp-685195) | 0.6768 | 0.000 | 5 |
KBiS(ClO2)2 (mp-23645) | 0.6744 | 0.000 | 5 |
KCaNd(PO4)2 (mp-676934) | 0.6632 | 0.000 | 5 |
CaGdTh(PO4)3 (mp-695308) | 0.6659 | 0.013 | 5 |
ErZr11Si11PO48 (mp-690951) | 0.6782 | 0.008 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tm_3 As O |
Final Energy/Atom-7.1443 eV |
Corrected Energy-182.7007 eV
-182.7007 eV = -171.4640 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)