Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.653 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.066 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaI2 + BaI2 |
Band Gap3.911 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/a [88] |
HallI 4bw 1bw |
Point Group4/m |
Crystal Systemtetragonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 199.9 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 139.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 333.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 266.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 139.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 66.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 333.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 66.6 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 266.5 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 139.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 266.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 333.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 333.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 266.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 66.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 333.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 133.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 333.2 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 139.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 139.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 333.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 66.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 333.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 139.6 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 197.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 266.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 66.6 |
Al (mp-134) | <1 1 0> | <1 0 0> | 139.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 333.2 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 133.3 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 333.2 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 199.9 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 333.2 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 333.2 |
C (mp-66) | <1 0 0> | <0 0 1> | 333.2 |
C (mp-66) | <1 1 0> | <1 1 0> | 197.5 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 133.3 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 139.6 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 333.2 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 66.6 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 266.5 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 333.2 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 266.5 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 333.2 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 133.3 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 0> | 139.6 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 333.2 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 333.2 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 66.6 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 333.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HfGeO4 (mp-9755) | 0.2373 | 0.000 | 3 |
CaZnF4 (mp-5104) | 0.1756 | 0.004 | 3 |
SrCaI4 (mp-850305) | 0.2231 | 0.090 | 3 |
DyWO4 (mp-769941) | 0.1564 | 0.071 | 3 |
LiYF4 (mp-3700) | 0.2539 | 0.000 | 3 |
LiCaUF8 (mp-632402) | 0.6627 | 0.025 | 4 |
Li2CaHfF8 (mp-16577) | 0.5282 | 0.000 | 4 |
TlCl2 (mp-27205) | 0.5286 | 0.000 | 2 |
TlBr2 (mp-27398) | 0.5876 | 0.000 | 2 |
InI2 (mp-29312) | 0.6253 | 0.000 | 2 |
InBr2 (mp-568108) | 0.6494 | 0.000 | 2 |
KF5 (mp-1095521) | 0.6435 | 0.094 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Ca_sv I |
Final Energy/Atom-3.3235 eV |
Corrected Energy-39.8823 eV
-39.8823 eV = -39.8823 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)