Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.946 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.027 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLu3Al5O12 + Lu2O3 |
Band Gap5.038 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 286.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 213.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 118.9 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 71.1 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 286.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 284.5 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 286.0 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 286.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 213.4 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 284.5 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 284.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 71.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 213.4 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 165.1 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 165.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 71.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 71.1 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 71.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 284.5 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 284.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 213.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 284.5 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 286.0 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 286.0 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 213.4 |
C (mp-66) | <1 0 0> | <1 0 0> | 190.7 |
C (mp-66) | <1 1 1> | <0 0 1> | 284.5 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 71.1 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 286.0 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 213.4 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 286.0 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 286.0 |
C (mp-66) | <1 1 0> | <1 0 0> | 286.0 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 213.4 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 284.5 |
PbSe (mp-2201) | <1 0 0> | <1 0 1> | 118.9 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 165.1 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 71.1 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 1> | 237.9 |
SiC (mp-11714) | <0 0 1> | <1 1 0> | 165.1 |
Si (mp-149) | <1 1 1> | <0 0 1> | 213.4 |
Au (mp-81) | <1 1 1> | <0 0 1> | 213.4 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 286.0 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 284.5 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 286.0 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 213.4 |
ZrO2 (mp-2858) | <0 0 1> | <1 1 0> | 165.1 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 286.0 |
YAlO3 (mp-3792) | <0 1 1> | <1 0 0> | 95.3 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 95.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La3ScO6 (mp-752569) | 0.1184 | 0.025 | 3 |
Li3AlH6 (mp-31096) | 0.1711 | 0.000 | 3 |
Gd3InO6 (mp-756715) | 0.2489 | 0.010 | 3 |
Ho3ScO6 (mp-13840) | 0.2238 | 0.000 | 3 |
Ca3UO6 (mp-14252) | 0.2346 | 0.000 | 3 |
Ca2NiWO6 (mvc-16546) | 0.3469 | 0.102 | 4 |
Mg2MoWO6 (mvc-5910) | 0.4214 | 0.033 | 4 |
Mg2CrWO6 (mvc-5960) | 0.4067 | 0.672 | 4 |
InNi2SbO6 (mp-1078367) | 0.4235 | 0.000 | 4 |
Ca3Zn3(TeO6)2 (mp-555961) | 0.4216 | 0.120 | 4 |
Fe2O3 (mp-777192) | 0.4560 | 0.732 | 2 |
Fe2O3 (mp-715572) | 0.4573 | 0.116 | 2 |
Fe2O3 (mp-686969) | 0.4485 | 0.071 | 2 |
Al2O3 (mp-776475) | 0.4206 | 0.030 | 2 |
Cr2O3 (mp-776873) | 0.4436 | 0.042 | 2 |
Li4Fe2TeWO12 (mp-768021) | 0.5354 | 0.083 | 5 |
CaLaFeBiO6 (mvc-8967) | 0.6673 | 0.057 | 5 |
Li4Cr2TeWO12 (mp-775566) | 0.6474 | 0.080 | 5 |
Li4Mn2TeWO12 (mp-768044) | 0.6217 | 0.056 | 5 |
Li4V2CrTeO12 (mp-775632) | 0.6483 | 0.104 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Lu_3 Al O |
Final Energy/Atom-8.2246 eV |
Corrected Energy-172.9187 eV
-172.9187 eV = -164.4913 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)