Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.279 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.81 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.941 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 275.5 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 239.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 127.5 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 298.9 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 231.1 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 139.4 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 220.0 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 231.1 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 59.8 |
KCl (mp-23193) | <1 1 1> | <1 1 -1> | 292.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 254.9 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 139.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 339.9 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 254.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 339.9 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 69.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 212.4 |
Te2W (mp-22693) | <0 1 1> | <1 0 -1> | 231.1 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 297.4 |
TePb (mp-19717) | <1 1 1> | <1 1 -1> | 292.6 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 209.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 212.4 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 127.5 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 298.9 |
BN (mp-984) | <1 0 0> | <0 0 1> | 339.9 |
BN (mp-984) | <1 1 1> | <1 0 -1> | 308.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 169.9 |
MoS2 (mp-1434) | <1 1 0> | <1 0 -1> | 231.1 |
Al (mp-134) | <1 1 0> | <1 0 0> | 69.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 293.4 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 179.4 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 169.9 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 0> | 209.1 |
Fe3O4 (mp-19306) | <1 1 1> | <1 0 1> | 257.8 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 169.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 169.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 169.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 254.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 171.9 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 209.1 |
KCl (mp-23193) | <1 1 0> | <1 1 -1> | 292.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 278.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 278.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 278.7 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 209.1 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 169.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 69.7 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 85.9 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 293.4 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 154.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hg2SeO5 (mp-30123) | 0.6005 | 0.000 | 3 |
Li3Fe(BO2)5 (mp-761304) | 0.6706 | 0.132 | 4 |
Sn2PCO6 (mp-559291) | 0.6701 | 0.028 | 4 |
CaGaBO4 (mp-557855) | 0.5926 | 0.000 | 4 |
CaAlBO4 (mp-559759) | 0.6511 | 0.000 | 4 |
K6Be4C6O19 (mp-555866) | 0.6291 | 0.000 | 4 |
Na2SbPCO7 (mp-768144) | 0.3578 | 0.000 | 5 |
Na2AsPCO7 (mp-767546) | 0.3397 | 0.010 | 5 |
Li2CuCSO7 (mp-771969) | 0.4318 | 0.077 | 5 |
Li2AsPCO7 (mp-768153) | 0.4334 | 0.064 | 5 |
Na2SbAsCO7 (mp-771166) | 0.3257 | 0.009 | 5 |
Li12Mn3CrP4(CO7)4 (mp-767734) | 0.6567 | 0.056 | 6 |
Li6MnCrP2(CO7)2 (mp-767287) | 0.6543 | 0.062 | 6 |
NaLiMnPCO7 (mp-763833) | 0.5938 | 0.062 | 6 |
NaLi5Mn2P2(CO7)2 (mp-773351) | 0.6547 | 0.070 | 6 |
NaLi5Mn2P2(CO7)2 (mp-774194) | 0.6167 | 0.249 | 6 |
CdRe2H16C4S4(NO)8 (mp-733747) | 0.7276 | 0.089 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Sb P C O |
Final Energy/Atom-6.5048 eV |
Corrected Energy-165.7324 eV
Uncorrected energy = -156.1144 eV
Composition-based energy adjustment (-0.687 eV/atom x 14.0 atoms) = -9.6180 eV
Corrected energy = -165.7324 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)