material

LiCoS2

ID:

mp-757100

DOI:

10.17188/1290705


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.042 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.049 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.44 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CoS2 + Co3S4 + Li2S
Band Gap
0.714 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3m [160]
Hall
R 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KCl (mp-23193) <1 1 1> <0 0 1> 0.000 70.8
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.000 131.5
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.000 70.8
Ni (mp-23) <1 1 1> <0 0 1> 0.002 192.2
ZnO (mp-2133) <0 0 1> <0 0 1> 0.005 121.4
BN (mp-984) <0 0 1> <0 0 1> 0.006 70.8
AlN (mp-661) <1 0 0> <1 1 0> 0.007 110.3
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.008 110.3
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.009 192.2
Au (mp-81) <1 0 0> <0 0 1> 0.012 192.2
TiO2 (mp-2657) <1 1 1> <1 0 1> 0.012 322.3
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.012 70.8
NaCl (mp-22862) <1 1 0> <1 0 1> 0.013 322.3
CdS (mp-672) <1 0 0> <0 0 1> 0.020 202.4
C (mp-48) <1 0 1> <1 0 1> 0.022 257.9
Au (mp-81) <1 1 1> <0 0 1> 0.025 30.4
AlN (mp-661) <1 1 1> <0 0 1> 0.031 172.0
ZrO2 (mp-2858) <1 1 0> <1 0 1> 0.032 322.3
SiC (mp-8062) <1 1 1> <0 0 1> 0.052 131.5
Mg (mp-153) <1 0 0> <0 0 1> 0.053 283.3
ZnO (mp-2133) <1 0 1> <1 0 0> 0.053 254.7
CdTe (mp-406) <1 0 0> <0 0 1> 0.055 354.1
AlN (mp-661) <1 1 0> <0 0 1> 0.058 273.2
BN (mp-984) <1 1 1> <0 0 1> 0.069 273.2
Ag (mp-124) <1 1 1> <0 0 1> 0.074 30.4
ZnSe (mp-1190) <1 1 0> <1 0 1> 0.075 322.3
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.087 110.3
SiO2 (mp-6930) <1 1 0> <1 0 1> 0.098 193.4
Ga2O3 (mp-886) <0 1 0> <0 0 1> 0.108 70.8
SiC (mp-7631) <1 0 1> <0 0 1> 0.111 192.2
Cu (mp-30) <1 0 0> <0 0 1> 0.142 212.5
Ag (mp-124) <1 1 0> <0 0 1> 0.154 121.4
SiC (mp-11714) <1 0 0> <0 0 1> 0.158 253.0
CeO2 (mp-20194) <1 0 0> <1 0 1> 0.175 322.3
CdWO4 (mp-19387) <1 0 1> <1 1 0> 0.183 220.6
Si (mp-149) <1 0 0> <1 0 1> 0.183 322.3
Al (mp-134) <1 0 0> <0 0 1> 0.191 182.1
Au (mp-81) <1 1 0> <0 0 1> 0.211 121.4
BaF2 (mp-1029) <1 1 0> <0 0 1> 0.216 283.3
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.223 263.1
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.232 141.7
Al2O3 (mp-1143) <1 0 1> <0 0 1> 0.238 323.8
GaN (mp-804) <1 0 0> <0 0 1> 0.240 283.3
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.245 293.4
TiO2 (mp-390) <1 0 0> <0 0 1> 0.254 182.1
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.255 182.1
CdWO4 (mp-19387) <0 1 0> <0 0 1> 0.259 313.7
C (mp-66) <1 1 0> <0 0 1> 0.263 202.4
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.263 273.2
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.270 161.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
158 44 30 -2 0 0
44 158 30 2 0 0
30 30 126 0 0 0
-2 2 0 1 0 0
0 0 0 0 1 -2
0 0 0 0 -2 57
Compliance Tensor Sij (10-12Pa-1)
7.3 -2 -1.3 16.6 0 0
-2 7.3 -1.3 -16.6 0 0
-1.3 -1.3 8.5 0 0 0
16.6 -16.6 0 1058.3 0 0
0 0 0 0 1058.3 33.2
0 0 0 0 33.2 18.6
Shear Modulus GV
34 GPa
Bulk Modulus KV
72 GPa
Shear Modulus GR
2 GPa
Bulk Modulus KR
70 GPa
Shear Modulus GVRH
18 GPa
Bulk Modulus KVRH
71 GPa
Elastic Anisotropy
69.63
Poisson's Ratio
0.38

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
NiAgTe2 (mp-976804) 0.2107 0.117 3
FeCuS2 (mp-1096975) 0.2489 0.128 3
CrAgTe2 (mp-1018084) 0.1674 0.043 3
CrCuS2 (mp-554579) 0.3271 0.038 3
YAgS2 (mp-1096795) 0.3141 0.015 3
CoAs2 (mp-2715) 0.7178 0.000 2
MnP4 (mp-571193) 0.7174 0.001 2
TcP4 (mp-28026) 0.7339 0.000 2
P3Ru (mp-28400) 0.5742 0.000 2
MnP4 (mp-569522) 0.7075 0.000 2
NaZr2SN2Cl (mp-679669) 0.6582 0.077 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv Co S
Final Energy/Atom
-5.0331 eV
Corrected Energy
-21.4594 eV
-21.4594 eV = -20.1325 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)